Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 5.40 MPa
783 psi
ASTM D412
Polymax® Maxelast® P2775 TPE, PP Overmold or Standalone use
Characteristics: Soft, flexible feelExcellent grip characteristicsGood weatherabilityGood compression setEasy processability and colorabilityAvailable FDA and medical gradesAvailable translucent gra..
Tensile Strength, Yield 5.40 MPa
783 psi
50% Elongation; ASTM D412
Covestro Texin® 5590 Thermoplastic Polyurethane, Polyether-based, Medical  (discontinued **)
This grade is in chemical compliance with 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber articles intended for repeated use) subject to the limitations of this regulation and any other r..
Tensile Strength, Yield 5.40 MPa

@Strain 100 %
783 psi

@Strain 100 %
ASTM D638
Toyobo A2080A Thermoplastic Polyurethane Elastomer, Injection Grade
Polycaprolactone type, featuring a good balance of mechanical strength and chemical resistance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe..
Tensile Strength, Yield 5.40 MPa

@Strain 100 %
783 psi

@Strain 100 %
ASTM D638
Toyobo A3080A Thermoplastic Polyurethane Elastomer, Injection Grade
Polyether type, featuring excellent resistance to hot water and fungus. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe soles, etc.Information ..
Tensile Strength, Yield 5.40 MPa
783 psi
50 microns film; ASTM D882
Arkema Group Orevac® 9318 Film EVA-MAH Terpolymer
EVA Terpolymers based Main Applications: Extrusion coating Thermo-adhesive filmsInformation provided by Arkema Group
Tensile Strength, Yield 5.40 MPa

@Strain 100 %
783 psi

@Strain 100 %
ASTM D638
Toyobo E2080A Thermoplastic Polyurethane Elastomer, Extrusion Grade
Polycaprolactone type, featuring a good balance of mechanical strength and chemical resistance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe..
Tensile Strength, Yield 5.40 MPa
783 psi
AVG Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 7168 Nitrile Rubber
Nitrile for oil & gas serviceInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield 5.40 MPa
783 psi
M100
3M Dyneon™ Fluorel™ FLS-2650 Fluoroelastomer VF2 + HFP + TFE Terpolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 70.3%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 1.8% Luperco™ 101XL Peroxide, and 2.5 % Triallyl ..