| Toyobo A2080A Thermoplastic Polyurethane Elastomer, Injection Grade |
Thermoplastic Polyurethane, Elastomer, Polyester Grade |
|
| Toyobo A1071D Thermoplastic Polyurethane Elastomer, Injection Grade |
Polyurethane, TP |
|
| Toyobo E2090A Thermoplastic Polyurethane Elastomer, Extrusion Grade |
Thermoplastic Polyurethane, Elastomer, Polyester Grade |
|
| Toyobo GLAMIDE® T-403 Nylon-6 |
Nylon 6, 50% Glass Fiber Filled |
GLAMIDE®
|
| Toyobo GLAMIDE® T-422-02 Nylon-6 |
Nylon 6, 40% Mineral Filled |
GLAMIDE®
|
| Toyobo GLAMIDE® T-663G30 Nylon-66 |
Nylon 66, 30% Glass Fiber Filled |
GLAMIDE®
|
| Toyobo GLAMIDE® T-663G50A MXD66 |
Nylon, Aromatic |
GLAMIDE®
|
| Toyobo GLAMIDE® T-714E Transparent Nylon |
Nylon, Aromatic |
GLAMIDE®
|
| Toyobo GLAMIDE® TY-102ND Nylon/Elastomer |
Nylon |
GLAMIDE®
|
| Toyobo GLAMIDE® TY-791GT 6T-Nylon |
Nylon, Aromatic |
GLAMIDE®
|
| Toyobo GLAMIDE® TY-791HT 6T-Nylon |
Nylon, Aromatic |
GLAMIDE®
|
| Toyobo GLAMIDE® TY-835TC Nylon-66 |
Nylon 66, 20% Mineral Filled |
GLAMIDE®
|
| Toyobo PELPRENE™ P150B-05 Polyester TPE, Non-smell, Non-deposit |
Polyester TPE |
Pelprene™
|
| Toyobo Pelprene™ P-150M Polyester TPE |
Polyether Ester Elastomer |
Pelprene™
|
| Toyobo Pelprene™ P-280B Polyester TPE |
Polyether Ester Elastomer |
Pelprene™
|
| Toyobo PELPRENE™ P40U Polyester TPE, Weather-resistant |
Polyester TPE |
Pelprene™
|
| Toyobo PELPRENE™ P46D-01 Polyester TPE, High Viscous, High Durability |
Polyester TPE |
Pelprene™
|
| Toyobo PELPRENE™ P90B Polyester TPE |
Polyester TPE |
Pelprene™
|
| Toyobo PELPRENE™ S2001 Polyester TPE |
Polyester TPE |
Pelprene™
|
| Toyobo PELPRENE™ S2002FB Polyester TPE, Flame Resistant |
Polyester TPE |
Pelprene™
|
| Toyobo PELPRENE™ S3001 Polyester TPE |
Polyester TPE |
Pelprene™
|
| Toyobo PELPRENE™ S9002 Polyester TPE, Ultra Heat-resistant |
Polyester TPE |
Pelprene™
|
| Toyobo T-400 Nylon, 15% Glass-Reinforced |
Nylon |
|
| Toyobo T-423 Nylon, Mineral-Reinforced |
Nylon |
|
| Toyobo T-750 Nylon, Painting Grade |
Nylon |
|
| Toyobo TS501 PPS, 50% Glass Fiber Reinforced |
Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler |
|
| Toyobo VYLOPET® CA5310 PC/PBT Polymer Alloy, High Rigidity, Impact Resistant |
Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced |
VYLOPET®
|
| Toyobo Vylopet® EMC120S Glass Reinforced Polyester, Standard Grade |
Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant |
VYLOPET®
|
| Toyobo Vylopet® EMC130-01 Glass Reinforced Polyester, Standard Grade |
Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant |
VYLOPET®
|
| Toyobo Vylopet® EMC130-04 Glass Reinforced Polyester, Easy Molding Grade |
Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant |
VYLOPET®
|
| Toyobo VYLOPET® EMC130-20 Injection Molding Polyester Resin, Flame Resistant |
Polyethylene Terephthalate (PET) |
VYLOPET®
|
| Toyobo VYLOPET® EMC317A Injection Molding Polyester Resin, Warpageless |
Polyethylene Terephthalate (PET) |
VYLOPET®
|
| Toyobo Vylopet® EMC330K Glass Reinforced Polyester, Easy Molding Grade |
Polyethylene Terephthalate (PET) |
VYLOPET®
|
| Toyobo VYLOPET® EMC333 Injection Molding Polyester Resin, Hydrolysis Resistant |
Polyethylene Terephthalate (PET) |
VYLOPET®
|
| Toyobo VYLOPET® EMC355 Injection Molding Polyester Resin, Glass Reinforced |
Polyethylene Terephthalate (PET) |
VYLOPET®
|
| Toyobo Diaflora® AS 1670B |
Polyether Ester Elastomer |
Diaflora®
|
| Toyobo Diaflora® ES 2220B |
Polyether Ester Elastomer |
Diaflora®
|
| Toyobo T-661 Nylon 66, Standard Grade (DAM) |
Nylon 66, Unreinforced |
|
| Toyobo Vylopet® EMC405A PET/PBT Blend |
PET + PBT Unreinforced |
VYLOPET®
|
| Toyobo Vylopet® EMC415 PET/PBT Blend |
PET + PBT Unreinforced |
VYLOPET®
|
| Toyobo Vylopet® EMC430 PET/PBT Blend |
Polybutylene Terephthalate (PBT) |
VYLOPET®
|
| Toyobo Vylopet® EMC630 PET/PBT Blend |
Polybutylene Terephthalate (PBT) |
VYLOPET®
|
| Toyobo Zylon® AS Poly(p-phenylene-2,6-benzobisoxazole) Fiber |
Thermoset |
Zylon®
|
| Toyobo Zylon® HM Fiber/Epoxy Matrix Unidirectional Composite |
Carbon Fiber/Thermoset Composite |
Zylon®
|
| Toyobo Zylon® HM Poly(p-phenylene-2,6-benzobisoxazole) Fiber |
Thermoset |
Zylon®
|
| Toyobo Diaflora® DS 2220B |
Polyether Ester Elastomer |
Diaflora®
|
| Toyobo GLAMIDE® T-401 Nylon-6 |
Nylon 6, 20% Glass Fiber Filled |
GLAMIDE®
|
| Toyobo PELPRENE™ P40B Polyester TPE |
Polyester TPE |
Pelprene™
|
| Toyobo Vylopet® EMC120K Glass Reinforced Polyester, Easy Molding Grade |
Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant |
VYLOPET®
|