Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 39.0 MPa
5660 psi
5 mm/min
Polimeri Europa EDISTIR N1841 Polystyrene  (discontinued **)
Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,085-12 General purpose polystyrene combining easy flow and medium heat. This grade exhibits excellent processability in ..
Tensile Strength, Ultimate 39.0 MPa
5660 psi
ASTM D638
Ineos Nova 3930 General Purpose Crystal Polystyrene  (discontinued **)
High melt flow, Crystal clearApplications: Razor components, Personal care, Thin wall moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and ..
Tensile Strength, Ultimate 39.0 MPa

@Temperature 60.0 °C
5660 psi

@Temperature 140 °F
ISO 527
LATI LATAN 13 Medium Viscosity Polyoxymethylene Copolymer (POM)  (Unverified Data**)
Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea..
Tensile Strength, Ultimate 39.0 - 68.0 MPa
5660 - 9860 psi
Average value: 52.0 MPa Grade Count:43
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Tensile Strength, Ultimate 39.0 MPa
5660 psi
ASTM D638
Ineos ABS Triax® 1220 S ABS + Polyamide Blend, Extrusion, Dry as Extruded
Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with
Tensile Strength, Ultimate 39.0 MPa
5660 psi
ASTM D638
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, Dry as Molded
Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi..
Tensile Strength, Ultimate 39.0 MPa
5660 psi
20 in/min, at max load; ASTM D412
A. Schulman POLYPUR™ FPU 1117 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Tensile Strength, Ultimate 39.0 MPa
5660 psi
20 in/min, at max load; ASTM D412
A. Schulman POLYPUR™ FPU 1117 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Tensile Strength, Ultimate 39.0 MPa
5660 psi
ASTM D638
Plenco 08112 Polyester BMC, Compression Molded
PLENCO 08112 is a renumber of PlasGlas 10112. PLENCO 08112 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co..
Tensile Strength, Ultimate 39.0 MPa
5660 psi
20 in/min, at max load; ASTM D412
A. Schulman POLYPUR™ FPU 1117 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Tensile Strength, Ultimate 39.0 MPa
5660 psi
20 in/min, at max load; ASTM D412
A. Schulman POLYPUR™ FPU 1117 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Tensile Strength, Ultimate 39.0 MPa
5660 psi
ASTM D638
Toyobo E3090A Thermoplastic Polyurethane Elastomer, Extrusion Grade
Polyether type, featuring excellent resistance to hot water and fungus. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe soles, etc.Information ..
Tensile Strength, Ultimate 39.0 MPa
5660 psi
20 in/min, at max load; ASTM D412
A. Schulman POLYPUR™ FPU 1117 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Tensile Strength, Ultimate 39.0 MPa
5660 psi
20 in/min, at max load; ASTM D412
A. Schulman POLYPUR™ FPU 1117 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Tensile Strength, Ultimate 39.0 MPa
5660 psi
DIN 53504
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tensile Strength, Ultimate 39.0 MPa
5660 psi
ASTM D638
Toyobo A3080A Thermoplastic Polyurethane Elastomer, Injection Grade
Polyether type, featuring excellent resistance to hot water and fungus. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe soles, etc.Information ..
Tensile Strength, Ultimate 39.0 MPa
5660 psi
DIN 53504
Lubrizol ESTANE® 58201 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tensile Strength, Ultimate 39.0 MPa
5660 psi
ASTM D638/D412
Covestro Baydur® GS-772 Polyurethane Solid RIM, MDI-based 2-Component Liquid System
0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of..
Tensile Strength, Ultimate 39.0 MPa
5660 psi
ASTM D638
Arkema Group PLATAMID® 8020 Copolyamide
Platamid® 8020 is a transparent, thermoplastic copolyamide designed for conversion by standard molding or extrusion techniques.Information provided by Arkema Group
Tensile Strength, Ultimate 39.0 MPa
5660 psi
ASTM D412
BASF Elastollan® C-85A Polyester Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen..
Tensile Strength, Ultimate 39.0 MPa
5660 psi
Abatron AboCast 8103-11 One Part Epoxy
One component system. Information provided by Abatron, Inc.Processing: Shelf life 6-8 months at 25°C (77°F). Heat cured; Pot life 190 min. at 100°C (212°C). Peak exotherm 170°C (340°F). At..
Tensile Strength, Ultimate 39.0 MPa
5650 psi
after optimum cure
Armstrong A-3/E Epoxy Adhesive
A Jet black epoxy paste especially formulated for bonding rigid materials. When used with Activator A or E, A-3 exhibits excellent bonding properties to phenolics, precious stones, ceramics, glass,..
Tensile Strength, Ultimate 39.0 MPa
5660 psi
ASTM D638
Solvay Specialty Polymers Algoflon® 1.2CSC PTFE; Superconductive Carbon Filled  (discontinued **)
Data provided by the manufacturer.1.2 wt.% Superconductive Carbon. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric prope..
Tensile Strength, Ultimate 39.0 MPa
5660 psi
ASTM D638
Toyobo E3080A Thermoplastic Polyurethane Elastomer, Extrusion Grade
Polyether type, featuring excellent resistance to hot water and fungus. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe soles, etc.Information ..
Tensile Strength, Ultimate 39.0 MPa
5660 psi
Z direction; ASTM D638
ALM D80-ST Nylon 11 SLS Prototyping Polymer
Unfilled, color stabilized nylon 11 material that is also stabilized to prevent premature thermal degradation. Parts produced from PA D80-ST exhibit superior mechanical properties. Relatively inexp..
Tensile Strength, Ultimate 39.0 MPa
5660 psi
ASTM D412
BASF Elastollan® S64D Polyester Type Polyurethane Elastomer
Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solv..
Tensile Strength, Ultimate 39.0 MPa
5660 psi
DIN 53504
Lubrizol ESTANE® 58437 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..