Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
Polymax® Maxelast® C4870 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
Polymax® Maxelast® C4960M TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
Polymax® Maxelast® C4975 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
Polymax® Maxelast® D6970 TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
Polymax® Maxelast® P2955T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
Polymax® Maxelast® C4950E TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
Polymax® Maxelast® C4990 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
Polymax® Maxelast® P1930D TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM 792 |
Multibase Multi-Flex® D 3902 MRS TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection tem.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-1377A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 1247-01 is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness. ApplicationPolypropylene PP 12.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1255-01 Polypropylene General Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1255-01 Natural is a general purpose molding grade, with UL 94 HB approval, homopolymer polypropylene. ApplicationPolypropylene PP 1255-01 meets FDA Regulation 21 CFR 177.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1255-01 Polypropylene General Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1255-01 Natural is a general purpose molding grade, with UL 94 HB approval, homopolymer polypropylene. ApplicationPolypropylene PP 1255-01 meets FDA Regulation 21 CFR 177.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 1247-01 is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness. ApplicationPolypropylene PP 12.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1255-01 Polypropylene General Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1255-01 Natural is a general purpose molding grade, with UL 94 HB approval, homopolymer polypropylene. ApplicationPolypropylene PP 1255-01 meets FDA Regulation 21 CFR 177.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection tem.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ISO 1183 |
Total Lumicene® MR10MX0 Metallocene Random Copolymer Polypropylene, Injection Molding and Injection Blow Molding Lumicene® MR10MX0 is a metallocene random copolymer with a melt flow index of 10 g/10 min for injection and injection stretch blow molding. Lumicene® MR10MX0 differs from the other random copolyme.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ISO 1183 |
Total PPM R020 Polypropylene, Random Copolymer for Medical Grade Polypropylene PPM R020 is a random copolymer polypropylene with a Melt Flow Index of 1.8 g/10 min specially developed for the extrusion blow molding of medical containers and medical devices, to the.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ISO 1183 |
Total PPR 10222 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 10222 is a nucleated and antistatic random copolymer polypropylene with a melt flow index of 40 g/10min for the injection molding of articles with high transparency and exce.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ISO 1183 |
Total PPR 12222 Random Copolymer Polypropylene Total Petrochemicals PPR 12222 is a high melt flow index, clarified random copolymer. Its high transparency makes it particularly suitable for the production of household articles and packaging. It.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1255-01 Polypropylene General Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1255-01 Natural is a general purpose molding grade, with UL 94 HB approval, homopolymer polypropylene. ApplicationPolypropylene PP 1255-01 meets FDA Regulation 21 CFR 177.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection tem.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ISO 1183 |
Total PPR 3261 Random Copolymer Polypropylene, Extrusion Grade Polypropylene PPR 3261 is a high melt strength random copolymer polypropylene with a melt flow index of 1.8 g/10 min suitable for extrusion applications.Information provided by Total Petrochemicals... |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ISO 1183 |
Total PPR 6288 Random Copolymer Polypropylene, Cast Extrusion of Film Total Petrochemicals PPR 6288 is a random copolymer polypropylene with a melt flow index of 8 g/10 min for the cast extrusion of films with outstanding optical properties and easy heat weldability.P.. |
|||
Specific Gravity | 0.902 g/cc | 0.902 g/cc | ASTM D792 |
E-Polymers EFLEX® V2060 SEBS/TPV V-series (Thermoplastic Vulcanizate Resins): E-FLEX V series resins are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic eq.. |