Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 67.0 °C @Load 5.001 kg |
153 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH T15010 H VTUV1 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 67.0 °C @Load 5.10 kg |
153 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Styrolution Styrolux BX6400 SBC Styrolux BX6400 is a developmental styrene butadiene copolymer (SBC) of high clarity and ultimate toughness used mainly in sheet and film extrusion and thermoforming applications. It is specifically.. |
|||
Vicat Softening Point | 67.0 °C @Load 5.10 kg |
153 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPM R020 Polypropylene, Random Copolymer for Medical Grade Polypropylene PPM R020 is a random copolymer polypropylene with a Melt Flow Index of 1.8 g/10 min specially developed for the extrusion blow molding of medical containers and medical devices, to the.. |
|||
Vicat Softening Point | 67.0 °C @Load 5.10 kg |
153 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPM R021 Polypropylene, Random Copolymer for Medical Grade Polypropylene PPM R021 is a random copolymer polypropylene with a Melt Flow Index of 1.8 g/10 min specially developed for the extrusion blow molding of medical containers and medical devices, to the.. |
|||
Vicat Softening Point | 67.0 °C @Load 5.10 kg |
153 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPR 10222 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 10222 is a nucleated and antistatic random copolymer polypropylene with a melt flow index of 40 g/10min for the injection molding of articles with high transparency and exce.. |
|||
Vicat Softening Point | 67.0 °C @Load 5.10 kg |
153 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPR 10232 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 10232 is a nucleated and antistatic random copolymer polypropylene with a melt flow index of 40 g/10min for the injection molding of articles with high transparency and exce.. |
|||
Vicat Softening Point | 67.0 °C @Load 5.10 kg |
153 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPR 12222 Random Copolymer Polypropylene Total Petrochemicals PPR 12222 is a high melt flow index, clarified random copolymer. Its high transparency makes it particularly suitable for the production of household articles and packaging. It.. |
|||
Vicat Softening Point | 67.0 °C @Load 5.10 kg |
153 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPR 12232 Random Copolymer Polypropylene Total Petrochemicals PPR 12232 is a high melt flow index, high transparency random copolymer. Its has an excellent food compatibility due to its low odor, making it especially suitable for the produ.. |
|||
Vicat Softening Point | 67.0 °C @Load 5.10 kg |
153 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPR 3221 Random Copolymer Polypropylene, Blow Molding and Sheet Extrusion Polypropylene PPR 3221 is a high clarity, high impact resistance random copolymer especially designed for blow molding applications (mono and multi-layers) for food and non-food packaging of sauces,.. |
|||
Vicat Softening Point | 67.0 °C @Load 5.10 kg |
153 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPR 7220 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 7220 is a nucleated random copolymer polypropylene with a melt flow index of 10 g/10 min for the injection molding of articles with high transparency and excellent surface a.. |
|||
Vicat Softening Point | 67.0 °C @Load 5.10 kg |
153 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPR 7227 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 7227 is a high transparency random copolymer polypropylene specially developed for the injection molding of caps and closures and articles with high transparency, excellent .. |
|||
Vicat Softening Point | 67.0 °C @Load 5.10 kg |
153 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPR 9220 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 9220 is a nucleated random copolymer polypropylene with a melt flow index of 20 g/10 min for the injection molding of articles with high transparency and excellent surface a.. |
|||
Vicat Softening Point | 67.0 °C @Load 5.10 kg |
153 °F @Load 11.2 lb |
ISO 306 |
Borealis Daplen™ EF267AI Polypropylene TPO Compound Daplen™ EF267AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |
|||
Vicat Softening Point | 67.0 °C @Load 5.10 kg |
153 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPR 3261 Random Copolymer Polypropylene, Extrusion Grade Polypropylene PPR 3261 is a high melt strength random copolymer polypropylene with a melt flow index of 1.8 g/10 min suitable for extrusion applications.Information provided by Total Petrochemicals... |
|||
Vicat Softening Point | 67.0 °C @Load 5.10 kg |
153 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPR 6280 Random Copolymer Polypropylene, Cast Film Extrusion Grade Total Petrochemicals PPR 6280 is a random copolymer polypropylene with a melt flow index of 7 g/10 min suitable for the cast extrusion of films with outstanding optical properties and easy heat weld.. |
|||
Vicat Softening Point | 67.0 °C @Load 5.10 kg |
153 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPR 6288 Random Copolymer Polypropylene, Cast Extrusion of Film Total Petrochemicals PPR 6288 is a random copolymer polypropylene with a melt flow index of 8 g/10 min for the cast extrusion of films with outstanding optical properties and easy heat weldability.P.. |
|||
Vicat Softening Point | 67.0 °C @Load 5.10 kg |
153 °F @Load 11.2 lb |
ISO 306 |
Addcomp PRIEX® 12031 Maleic Anhydride Grafted HDPE Fields of application: Functionalised polyethylene to be used as compatibiliser for polymer blends or coupling agent for wood flour, natural fibres, or mineral filled polyolefins. Also suitable to r.. |
|||
Vicat Softening Point | 67.0 °C @Load 5.10 kg |
153 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPR 3260 Random Copolymer Polypropylene, Extrusion Grade Polypropylene PPR 3260 is a random copolymer polypropylene with a melt flow index of 1.8 g/10 min suitable for extrusion applications.Information provided by Total Petrochemicals. |