Polymer Property : Flexural Modulus = 131 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.900 GPa
131 ksi
ASTM D790
Reliance Industries Relene M60075 Polyethylene
Relene M60075 is a High Density Polyethylene grade suitable for injection molding applications where good mechanical properties, gloss, dimensional stability, and good ESCR are required. This grade..
Flexural Modulus 0.900 GPa
131 ksi
3 pt. secant. ASTM D790
Chevron Phillips HiD® 9398T HDPE Natural Pipe Resin  (discontinued **)
Resin Type: Linear Copolymer; ASTM D 3350 Classification: 345420A; ASTM D 4976 Classification: PE 235, A 56601Applications:Base Resin for use in Utility and Conduit Pipe ApplicationsData provided by..
Flexural Modulus 0.900 GPa
131 ksi
3 pt. secant. ASTM D790
Chevron Phillips HiD® 9646T HDPE High Molecular Weight Sheeting Resin  (discontinued **)
Resin Type: Linear Copolymer; ASTM D 4976 Classification: PE 235, A 56606Applications:Sheeting, Thermoforming, Profile ExtrusionData provided by Chevron Chemical.
Flexural Modulus 0.900 GPa
131 ksi
ASTM D790
Reliance Industries Relene L60075 Polyethylene
Relene L60075 is UV stabilized. It is available with a recommended service life of more then 5 years L60075 is suitable for applications where articles are exposed to sunlight e.g. soft drink crates..
Flexural Modulus 0.900 GPa
131 ksi
2 mm/min; ISO 178
Inno-Comp INNOPOL® CS 2-3302 TO BU Elastomer Modified, UV-Stabilized Polypropylene Block-Copolymer
INNOPOL® CS 2-3302 TO BU is an elastomer modified, UV-stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-3302 TO BU is developed for producing injection molded automotive..
Flexural Modulus 0.900 GPa
131 ksi
ASTM D790
Kaneka PHBH Semi-Rigid Bio-based Polymer
A copolymer produced of 3-hydroxybutyrate and 3-hydroxyhexanoate produced by fermentation of plant oils. It has excellent biodegradability (under anaerobic, aerobic, aquatic, and compost conditions..
Flexural Modulus 0.903 GPa
131 ksi
ISO 178
LyondellBasell Hifaxâ„¢ CB272 Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CB272 high melt flow, 900 MPa flexural modulus, low CLTE, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of rigidity and dime..
Flexural Modulus 0.900 GPa
131 ksi
ISO 178
Styrolution Styrolux BX6400 SBC
Styrolux BX6400 is a developmental styrene butadiene copolymer (SBC) of high clarity and ultimate toughness used mainly in sheet and film extrusion and thermoforming applications. It is specifically..
Flexural Modulus 0.900 GPa
131 ksi
ASTM D790
SCG Chemicals EL-Leneâ„¢ H1000PBL High Density Polyethylene Pipe Resin
Key Characteristics: Good processing, high thermal stability, good resistance to weathering, good balance of MRS and SCGRecommended Applications: Water pressure pipes and stripe lines for PE100 pi..
Flexural Modulus 0.900 GPa
131 ksi
ASTM D790
A. Schulman POLYFORT™ PP 7001
Information provided by A. Schulman.
Flexural Modulus 0.900 GPa
131 ksi
2mm/min; ISO 178
Borealis EE002AE Polypropylene Elastomer Modified
EE002AE is a reactor elastomer modified polypropylene compound intended for injection molding. The product is available in natural color. This material has excellent balanced mechanical properties..
Flexural Modulus 0.900 GPa
131 ksi
ISO 178
Unipetrol PE HD LITEN® LS 87 HDPE
Made for special applicationsInformation provided by Unipetrol RPA
Flexural Modulus 0.900 GPa
131 ksi
ISO 178
Unitika A1030BRL PA6, Conditioned
Information provided by Unitika Ltd.
Flexural Modulus 0.900 GPa
131 ksi
at 70°C, tangent
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Flexural Modulus 0.900 GPa
131 ksi
at 70°C, tangent
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Flexural Modulus 0.900 GPa
131 ksi
ISO 179
Total PPM R020 Polypropylene, Random Copolymer for Medical Grade
Polypropylene PPM R020 is a random copolymer polypropylene with a Melt Flow Index of 1.8 g/10 min specially developed for the extrusion blow molding of medical containers and medical devices, to the..
Flexural Modulus 0.900 GPa
131 ksi
ISO 178
Total PPR 9220 Random Copolymer Polypropylene, Injection Molding
Total Petrochemicals PPR 9220 is a nucleated random copolymer polypropylene with a melt flow index of 20 g/10 min for the injection molding of articles with high transparency and excellent surface a..
Flexural Modulus 0.900 GPa
131 ksi
ISO 178
Unitika A1030SR PA6, Conditioned
Information provided by Unitika Ltd.
Flexural Modulus 0.900 GPa
131 ksi
ISO 178
Total PPR 3261 Random Copolymer Polypropylene, Extrusion Grade
Polypropylene PPR 3261 is a high melt strength random copolymer polypropylene with a melt flow index of 1.8 g/10 min suitable for extrusion applications.Information provided by Total Petrochemicals...
Flexural Modulus 0.900 GPa
131 ksi
at 70°C, tangent
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Flexural Modulus 0.900 GPa
131 ksi
3 pt. secant. ASTM D790
Chevron Phillips Marlex® 9346 HDPE Natural Pipe Resin
Resin Type: Linear Copolymer; PE3408 Pipe Resin; ASTM D 3350 Classification:345464C when used with an approved color concentrate; ASTM D 4976 Classification: PE 235, A 56607Applications:Pressure Pip..
Flexural Modulus 0.900 GPa
131 ksi
2% Secant; ASTM D790
Chevron Phillips Marlex® 9398 HDPE Pipe and Corrugated Extrusion Resin
Resin Type: Hexene CopolymerCharacteristics: Good melt strengthExcellent ESCRApplications: ConduitDuctInformation provided by Chevron Phillips.
Flexural Modulus 0.900 GPa
131 ksi
cond; ISO 178
DSM Stanyl® TW341-B PA46
Heat Stabilized, Lubricated
Flexural Modulus 0.903 GPa
131 ksi
Secant; ISO 178
ExxonMobil Exxtral™ BNT 010 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior painted parts such as bumper fascia.Availability: Africa & Middle East, Asia Pacific, Europe, South A..
Flexural Modulus 0.900 GPa
131 ksi
SAE J949
Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (5 mm Molded Thickness)
AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Modulus 0.900 GPa
131 ksi
ASTM D790
Asahi Glass Fluon® ETFE
A thermoplastic fluoropolymer developed by Asahi Glass. It is a copolymer comprising of tetrafluoroethylene and ethylene. Fluon® ETFE is a balanced fluoropolymer that has chemical resistance and el..
Flexural Modulus 0.900 GPa
131 ksi
ISO 178
Ascend Performance Materials Vydyne® 66R Nylon 66, General Purpose, high viscosity, Conditioned
Vydyne® 66R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66R resin offers high strength, ..
Flexural Modulus 0.900 GPa
131 ksi
STN EN ISO 178
Plastcom SLOVALEN PQ 51 N Polypropylene Homopolymer, Modified with Elastomer, Impacted
FeaturesHomopolymer PP modified with elastomer. The addition of thermoplastic elastomer causes increased toughness, possible alternative to PP copolymers. General application in all industry branc..
Flexural Modulus 0.900 GPa
131 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Solvay Engineered Polymers DEXFLEX® 980HF TPO  (discontinued **)
Description: DEXFLEX® 980HF is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require high flow for excellent processability, ductile impact prope..
Flexural Modulus 0.903 GPa
131 ksi
ISO 178
LyondellBasell Hifax™ ETA3163/1 Thermoplastic Polyolefin Elastomer
Description: Hifax™ ETA3163/1 medium melt flow, 900 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of stiffness and low temper..