Material Notes:
ATOFINA 4624WZ polypropylene is a nucleated impact copolymer, combining good fluidity and mechanical properties. 4624WZ is characterized by significantly improved resistance, while maintaining excellent antistatic properties and good processability.ApplicationATOFINA 4624WZ has been developed specifically for the injection molding of buckets, pails, toys, housewares and garden furniture. Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D1505
Melt Flow 13 g/10 min
13 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus 1.15 GPa
167 ksi
ASTM D 790
Izod Impact, Notched 2.00 J/cm
3.75 ft-lb/in
ASTM D256
0.650 J/cm

@Temperature -20.0 °C
1.22 ft-lb/in

@Temperature -4.00 °F
ASTM D256
Charpy Impact Unnotched 1.90 J/cm²
9.04 ft-lb/in²
Notched/Unnotched not specified; ASTM DIN53453
0.700 J/cm²

@Temperature -20.0 °C
3.33 ft-lb/in²

@Temperature -4.00 °F
Notched/Unnotched not specified; ASTM DIN53453
Thermal Properties Metric English Comments
Melting Point 160 - 165 °C
320 - 329 °F
ATOFINA Method
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
Vicat Softening Point 148 °C
298 °F
ASTM D1525