PolyChem Alloy FilmStat 3K2

Category Polymer , Film
Manufacturer PolyChem Alloy
Trade Name FilmStat
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyChem Alloy FilmStat 3K2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Antistat concentrate based on Lauramide in a LLDPE carrier. Available in pelletized form in 50 lb. Bags
Physical Properties Metric English Comments
Specific Gravity 1.00 - 1.20 g/cc
1.00 - 1.20 g/cc