Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.15 GPa | 167 ksi | STN EN ISO 178 |
Plastcom PLASTALEN® PC 69 T 10 003/1M Polypropylene reinforced with mineral filler Modified PP copolymer for injection molding with the content of 10% mineral filler. Application in all automotive industry. Delivered in black.Information Provided by Plastcom spol. s r.o. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | STN EN ISO 178 |
Plastcom PLASTALEN® PQ 82 N 003/1M Polypropylene with improved impact strength PP copolymer regranulate for injection molding, impact modified. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | Tangent; 1.3 mm/min; ASTM D790 |
Mytex Polymers AN16L(W)-D56 Polypropylene, Talc filled, Compounded, Elastomer, Impact modified Description: AN16L-D56 is a compounded talc filled elastomer modified polypropylene with good impact and excellent material flow properties.Key Applications: Automotive exteriorInformation provided .. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | Tangent; 1.3 mm/min; ASTM D790 |
Mytex Polymers AN16L-53 Polypropylene, Compounded Description: Compounded polypropylene produced for automotive exterior applications using Mytex® Technology.Key Applications: Body side moldingInformation provided by Mytex Polymers |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | Tangent; 1.3 mm/min; ASTM D790 |
Mytex Polymers AS33L-07V Polypropylene, Rubber modified, Compounded Description: AS33L-07 is a compounded, rubber modified polypropylene with good impact and excellent material flow properties. This product is designed for painted and mold-in-color applications.Key.. |
|||
Flexural Modulus | 1.15 GPa @Temperature 23.0 °C |
167 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYelast TPE EC12 D55 Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Flexural Modulus | >= 1.15 GPa | >= 167 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 8348S (EPH31RA) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | Tangent; ASTM D790 |
Flint Hills AP6112-HS Impact Copolymer Polypropylene High impact copolymer, UL certified, and FDA compliant. Features: Heat stabilizedApplications: Injection molding: appliance components, automotive interior trim, and consumer durables.Former Huntsma.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | 2 mm/min; ISO 178 |
Inno-Comp INNOPOL® CS 2-9301 Elastomer Modified Polypropylene Block-Copolymer INNOPOL® CS 2-9301 is an elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-9301 is developed for produ.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ISO 178 |
MRC Polymers MAXTEL™ 600T18 TPO, 18% Talc Filled • For automotive exterior applications• Excellent process ability and dimensional stability• Can be UV Stabilized• Internal and external lubricants can be addedInformation pr.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ISO 178 |
MRC Polymers MAXTEL™ 600T18-UV TPO, 18% Talc Filled, UV Stabilized • For automotive exterior applications• Excellent process ability and dimensional stabilityInformation provided by MRC Polymers Inc. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ISO 178 |
Ineos ABS Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade Triax® 1185 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with excellent processability, good chemical resistance, g.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ISO 178 |
Iran Petrochemical (PCC) EP-T 30 R Polypropylene The grade is a medium flow heterophasic the copolymer mainly designed for injection molding application.Application: containers, buckets, pails, crates and also used for automotive parts.Informatio.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY 63000CTC PC+POLYESTER (Asia Pacific) A permanent antistatic PC-Alloy compound that features transparency and superior cleanliness for advanced semiconductor packaging applications |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ISO 178-1975 |
SIDPEC EGYPTENE® HD 5211 EA HDPE Injection Molding Applications:Paint pailsBottle capsHouse waresToysInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Asia Pacific) Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | 2mm/min; ISO 178 |
Borealis Daplen™ EH104AE Polypropylene TPO Compound Daplen™ EH104AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, high.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ISO 178 |
Unipetrol PP MONSTEN® MA 611 Polypropylene Impact Copolymer Made for injection molding applications. Antistatic stabilization. Impact copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ISO 527-2 |
Total PPC 11712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 11712 is a nucleated controlled-rheology heterophasic copolymer. PPC 11712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ISO 527-2 |
Total PPC 3660 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 3660 is an heterophasic copolymer. PPC 3660 is characterized by a low fluidity hence good melt strength to provide east of processing and good manufactured article propert.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ISO 178 |
Total PPR 12232 Random Copolymer Polypropylene Total Petrochemicals PPR 12232 is a high melt flow index, high transparency random copolymer. Its has an excellent food compatibility due to its low odor, making it especially suitable for the produ.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | At 2 mm/min; ISO 178 |
Borealis Daplen™ EE015U TPO Compound Daplen EE015U is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE015U is a material with excellent impact /stiffness ratio. Thanks to its low th.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | 2% Secant; ASTM D790 |
Entec Hypel® PEHD18/.956 HDPE Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ASTM D790 |
Equate EMDA-8920 HDPE Injection Molding Resin EMDA-8920 is a high density copolymer polyethylene resin designed for injection molding applications which require excellent toughness and gloss.Applications: EMDA-8920 is a high density copolymer p.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B |
Dow DMDA-8920 NT 7 High Density Polyethylene Resin DOW DMDA-8920 NT 7 is produced using UNIPOL™ process technology. It is intended for use in a broad range of injection molding applications such as housewares, toys, food containers and pails. Info.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | SAE J949 |
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness) AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ASTM D790 |
Carmel Olefins CAPILENE® SE 50 E Polypropylene Impact Copolymer Description: CAPILENE® SE 50 E is a low melt flow rate impact copolymer intended for sheet extrusion. It exhibits excellent impact strength even at low temperatures, combined with good processabi.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ASTM D790 |
Carmel Olefins CAPILENE® SR 50 Polypropylene Impact Copolymer Description: CAPILENE® SR 50 is a medium melt flow rate impact copolymer for injection molding applications. This grade offers good balance of stiffness, impact strength and processability.Applic.. |
|||
Flexural Modulus | 1.15 GPa | 167 ksi | ISO 178 |
CENTROPLAST CENTROLAB HT Polypropylene Higher Temperatures PP-HT is a semi-crystalline plastic, with high acid and chemical resistance and mechanical strength. Due to its high resistance to temperature, PP-HT-plastics are often used in medical technology as.. |