Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.00 J/cm | 3.75 ft-lb/in | ASTM D256 |
NYCOA 5133 HS 33% Glass-Fiber Reinforced, Impact Modified, Heat Stabilized Nylon 66 Resin NYCOA 5133 HS is a 33% glass fiber reinforced, heat stabilized, impact modified, Nylon 66 suitable for injection molding. It offers excellent balance of mechanical, thermal and chemical properties; .. |
|||
Izod Impact, Notched | 2.00 J/cm | 3.75 ft-lb/in | ISO 180/A |
Polimeri Europa Eraclene® ML 74 High Density Polyethylene - Injection Molding Eraclene ML 74 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Its narrow molecular weight distribution leads to high mechanical properties .. |
|||
Izod Impact, Notched | 2.00 J/cm | 3.75 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
Izod Impact, Notched | 2.00 J/cm | 3.75 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS (Asia Pacific) Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
Izod Impact, Notched | 2.00 J/cm | 3.75 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS (Europe-Africa-Middle East) Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
Izod Impact, Notched | >= 2.00 J/cm @Temperature 23.0 °C |
>= 3.75 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PE 4850B (504H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Izod Impact, Notched | >= 2.00 J/cm @Temperature 23.0 °C |
>= 3.75 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PE 6748F (486H6) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Izod Impact, Notched | 2.00 J/cm @Temperature -40.0 °C |
3.75 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
LATI LASTANE 50 G/40 40% Glass Fiber Reinforced Polyurethane (PUR)
(discontinued **) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Izod Impact, Notched | 2.00 J/cm | 3.75 ft-lb/in | ASTM D256 |
Gichem GILAC E200 Acrylonitrile Butadiene Styrene
(discontinued **) ABS medium fluidity, excellent resilience. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Izod Impact, Notched | 2.00 J/cm | 3.75 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem GF 4960 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Izod Impact, Notched | 2.00 J/cm @Temperature -30.0 °C |
3.75 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER (Europe-Africa-Middle East) F-1 weathering certified in natural color, specially designed for Pool & Spa applications. Currently available in natural color only. |
|||
Izod Impact, Notched | 2.00 J/cm @Temperature -30.0 °C |
3.75 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Asia Pacific) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Izod Impact, Notched | 2.00 J/cm @Temperature -30.0 °C |
3.75 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Europe-Africa-Middle East) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Izod Impact, Notched | 2.00 J/cm | 3.75 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Izod Impact, Notched | 2.00 J/cm | 3.75 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS (Europe-Africa-Middle East) NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Izod Impact, Notched | 2.00 J/cm @Temperature -30.0 °C |
3.75 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Asia Pacific) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Izod Impact, Notched | 2.00 J/cm @Temperature -30.0 °C |
3.75 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Europe-Africa-Middle East) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Izod Impact, Notched | 2.00 J/cm | 3.75 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOTUF PX07437 PA 6 Compound based on Nylon 6 resin containing glass fiber and impact modifier. |
|||
Izod Impact, Notched | 2.00 J/cm | 3.75 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 2.00 J/cm | 3.75 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 2.00 J/cm @Temperature 23.0 °C |
3.75 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PB305G33 Nylon 6, 33% Glass Fiber 33% glass fiber reinforced, heat stabilized and UV stabilized polyamide 6 approved and listed by W.R.C and NSF/ANSI 61 international for potable waterInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.00 J/cm @Temperature 23.0 °C |
3.75 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron P40N01 Homopolymer Polypropylene, Chemically Coupled 40% Long Glass Fiber A CHEMICALLY COUPLED 40% LONG GLASS FIBER REINFORCED NATURAL POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.00 J/cm | 3.75 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 2.00 J/cm | 3.75 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 2.00 J/cm @Temperature 23.0 °C |
3.75 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron P40B01 Homopolymer Polypropylene, Chemically Coupled 40% LGF A chemically coupled 40% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.00 J/cm | 3.75 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® TB120G60W , 62% Glass Fiber Reinforced PA6, DAM High strength, weather resistanceInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 2.00 J/cm | 3.75 ft-lb/in | ISO 180 |
Azoty Tarnow™ TARFLEN SM-G20 PTFE Reinforced with 20% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Izod Impact, Notched | >= 2.00 J/cm | >= 3.75 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATS 166 Phenolic Molding Chopped cotton fabric Filler, Compression Molded Characteristics:High impact strengthGlossy surfaceLow shrinkageGood sliding propertiesColor-BlackMedium flowApplications:Cog wheelsCastor wheelsBush bearingsPulleysWelding rod handlesTextile bobbins.. |
|||
Izod Impact, Notched | 2.00 J/cm | 3.75 ft-lb/in | ASTM D256 |
Adell AJ-17 Nylon 66, 35% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 2.00 J/cm @Temperature 23.0 °C |
3.75 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LARIL 13 Light Brown Polyphenylene Oxide (PPOm)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |