Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastxWorld CEVIAN® B2706 30% GF PBT/ABS Alloy

Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyester Alloy + GF , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer PlastxWorld, Inc.
Trade Name CEVIAN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld CEVIAN® B2706 30% GF PBT/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass fiber reinforced PBT/ABS alloy.Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ASTM D792
Water Absorption 0.15 %
0.15 %
24 hr; ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 118 MPa
17100 psi
ASTM 638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 167 MPa
24200 psi
ASTM D790
Flexural Modulus 8.76 GPa
1270 ksi
ASTM D790
Izod Impact, Notched 0.747 J/cm

@Thickness 3.17 mm
1.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 36.0 µm/m-°C

@Temperature 20.0 °C
20.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ASTM D648
Flammability, UL94 HB
HB