ATOFINA Polypropylene PPC 3645 is a nucleated heterophasic copolymer. PPC 3645 is characterized by improved stiffness, creep resistance and high impact resistance.ApplicationPPC 3645 has been developed specifically for the extrusion of corrugated cardboard, corrugated and twin walled pipes, conduit pipe and other extrusion applications.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Bulk Density 0.525 g/cc
0.0190 lb/in³
ISO 1183
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Melt Flow 1.3 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.3 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 82
82
ISO 2039-2
Tensile Strength, Yield 29.0 MPa
4210 psi
ISO 527-2
Elongation at Yield 6.0 %
6.0 %
ISO 527-2
Tensile Modulus 1.50 GPa
218 ksi
ISO 527-2
Flexural Modulus 1.40 GPa
203 ksi
ISO 527-2
Izod Impact, Notched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
ISO 179
9.00 kJ/m²

@Temperature -20.0 °C
4.28 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
Low Temp; ISO 179
>= 5.00 J/cm²
>= 23.8 ft-lb/in²
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C
198 °F
120°C per hour; ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
120°C per hour; ISO 75-2
Vicat Softening Point 68.0 °C
154 °F
50N-50°C per hour; ISO 306
137 °C
279 °F
10N-50°C per hour; ISO 306