Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total Lacqtene® 2006 TN 35 HDPE pipe coating  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , MDPE , Medium Density Polyethylene (MDPE), Extruded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lacqtene® 2006 TN 35 HDPE pipe coating  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LACQTENE® 2006 TN 35 is a medium density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2006 TN 35 may be used for pipe and sheet extrusion (flexible sheets, membranes, liners,...)Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.936 g/cc
0.0338 lb/in³
ISO 1183
Thermal Stress Crack Resistance >= 1000 hour
>= 1000 hour
ASTM D 1693
Oxidative Induction Time (OIT) >= 20 min
>= 20 min
200°C; EN 728
Melt Flow 0.70 g/10 min

@Load 2.16 kg
0.70 g/10 min

@Load 4.76 lb
ISO 1133
2.7 g/10 min

@Load 5.00 kg
2.7 g/10 min

@Load 11.0 lb
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ISO 868
Tensile Strength, Yield 18.0 MPa
2610 psi
ISO 527-2
Elongation at Break >= 600 %
>= 600 %
ISO 527-2
Flexural Modulus 0.650 GPa
94.3 ksi
ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Melting Point 126 °C
259 °F
ISO 3146
Vicat Softening Point 114 °C
237 °F
ISO 306
Descriptive Properties Value Comments
Food Status This material conforms to both European and American Food contact regulations.
Users viewing this material also viewed the following: