Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 114 °C | 237 °F | Rate B; 4 mm thick;10.0 mm wide molded rod; ISO 306/B50 |
Premix Thermoplastics PRE-ELEC® ESD 7300 PRE-ELEC ESD 7300 is a static dissipative thermoplastic compound based on PC/PBT. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7300 has been developed for inj.. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Asia Pacific) Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by.. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Asia Pacific) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® ML7677A PC (Asia Pacific) Commercial grade for Polycarbonate in only nature color. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm.This data was supplied by SABIC-IP for the Asia Pacific reg.. |
|||
Vicat Softening Point | 114 °C | 237 °F | B; STN EN ISO 306 |
Plastcom SLOVALEN PC 53 N Polypropylene Copolymer, UV Stabilization FeaturesModified copolymer PP for injection moulding, with the ability of modeling the melt flow rate within the interval 5 - 20 g/10 min. Can be used for simple small as well as for large complica.. |
|||
Vicat Softening Point | 114 °C | 237 °F | ASTM D1525 |
SABIC R50035 Linear Low Density Polyethylene for Rotational Molding Product Description: R50035 are Linear Low Density Polyethylene grades designed to provide excellent stress crack resistance, mechanical properties with high rigidity, toughness, gloss and low warp.. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Vicat Softening Point | 114 °C | 237 °F | ASTM D1525 |
NOVA Chemicals Sclair® 8405 BK, 8405GBK MDPE Rotational Molding Resin
(discontinued **) Features: Good ESCR, high impact strength.Applications: Spray tanks.Data provided by the manufacturer. |
|||
Vicat Softening Point | 114 °C | 237 °F | ASTM D1525 |
NOVA Chemicals Sclair® 2515 MDPE Injection Molding Resin
(discontinued **) Features: Excellent processability for applications requiring moderate stiffness and improved toughnessExcellent cold temperature impact properties Applications: Ice cream containersHousewares Deep.. |
|||
Vicat Softening Point | 114 °C | 237 °F | ASTM D1525 |
Petroquimica Triunfo Trithene® TX 3003 LDPE - Shrink Wrap Film The Trithene® TX 3003 resin is a low-density polyethylene (LDPE) with high molecular weight, presenting excellent mechanical properties. The product provided elevated gloss and transparency, adding.. |
|||
Vicat Softening Point | 114 °C | 237 °F | ISO 306A |
Lucite International Diakon® ST25H8 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Asia Pacific) Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Asia Pacific) Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Europe-Africa-Middle East) Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
Vicat Softening Point | 114 °C | 237 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® HI-1001BN PC/ABS, Unreinforced PC/ABS that is used for the housing of mobile phone, wheel cap, rice cooker, electric iron etc., refrigerator door handle, panel etc.Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 114 °C | 237 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® HI-1001BN PC/ABS, Unreinforced PC/ABS that is used for the housing of mobile phone, wheel cap, rice cooker, electric iron etc., refrigerator door handle, panel etc.Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL EXNL0353 PPE+HIPS EXNL0353 resin is a modified PPE + PS blend with an excellent balance of non-halogenated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gravity for l.. |
|||
Vicat Softening Point | 114 °C | 237 °F | ISO 306 |
Borealis Bormed™ TD109CF Polypropylene Copolymer Bormed™ TD109CF is a propylene alpha olefin copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: lamination films, food.. |
|||
Vicat Softening Point | 114 °C | 237 °F | A50; ISO 306 |
Lubrizol ESTANE® GP92AT Ether Based Thermoplastic Polyurethane Type: Estane® GP 92AT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Vicat Softening Point | 114 °C | 237 °F | ISO 306 |
Total Lumicene® mPE M 2310 EP Metallocene Polyethylene, Blown Film Lumicene® mPE M 2310 EP is a second generation metallocene based Linear Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2310 EP can be processed at high output rates with low ext.. |
|||
Vicat Softening Point | 114 °C | 237 °F | |
Covestro Bayblend® KL 1-1430 Polycarbonate/ABS Blend Standard grade for cars.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Vicat Softening Point | 114 °C | 237 °F | ASTM D1525 |
Dow TUFLIN™ HS-7094 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7094 NT 7 is a fractional melt, ethylene-hexene copolymer, designe.. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Europe-Africa-Middle East) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Vicat Softening Point | 114 °C | 237 °F | B/120; ISO 306 |
Sax Polymers SAXALEN PPC344G25 Polypropylene Copolymer, 25% Glass Filled SAXALEN PPC344G25 is a 25% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers |
|||
Vicat Softening Point | 114 °C | 237 °F | under 1 daN; ASTM D1525 |
Arkema Group Pebax® MX 1205 Polyether Block Amide (PEBA) Typical application: Impact modifierInformation provided by Arkema Group |