Physical Properties Metric English Comments
Melt Flow 2.7 g/10 min

@Load 5.00 kg
2.7 g/10 min

@Load 11.0 lb
ISO 1133
Total Lacqtene® 2006 PBK 35 HDPE pipe, sheet  (discontinued **)
LACQTENE® 2006 PBK 35 is a medium density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2006 PBK 35 may be used for pipe extrusion (micro-irriga..
Melt Flow 2.7 g/10 min

@Load 5.00 kg
2.7 g/10 min

@Load 11.0 lb
ISO 1133
Total Lacqtene® 2006 TN 35 HDPE pipe coating  (discontinued **)
LACQTENE® 2006 TN 35 is a medium density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2006 TN 35 may be used for pipe and sheet extrusion (flex..
Melt Flow 2.7 g/10 min

@Load 21.6 kg,
Temperature 190 °C
2.7 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Iran Petrochemical (PCC) BL6 HM7255 High Density Polyethylene
BL6 (HM 755) is a high density polyethylene with Butene-1 as a comonomer. It is a high molar mass material with very good impact strength, stiffness, and stress cracking resistance.Applications: la..
Melt Flow 2.7 g/10 min

@Load 21.6 kg,
Temperature 190 °C
2.7 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Iran Petrochemical (PCC) BL 3VD HH 4765 High Density Polyethylene
BL3VD is a high density polyethylene with 1-Butene as co monomer. It is very high density and stiffness, good ESCR, high flowability and impact strength.Applications: small blow molding, bottles, c..
Melt Flow 2.7 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.7 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Topas Advanced Polymers TOPAS® Elastomer E-140 Developmental Cyclic Olefin Copolymer (COC)
TOPAS® Elastomer E-140, unlike most TOPAS grades, is a semicrystalline cyclic olefin material with flexibility. It is a fairly stiff elastomer which can be extruded and injection molded, and can be..
Melt Flow 2.7 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.7 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Denka CL-430 Transparent Resin Polymer (MABS) ABS
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Melt Flow 2.7 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.7 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Denka TE-20 Transparent Resin Polymer (MABS resin) ABS
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Melt Flow 2.7 g/10 min

@Load 3.80 kg,
Temperature 230 °C
2.7 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ABS TR-7
Description: High Heat ABSInformation provided by Diamond Polymers, Inc.
Melt Flow 2.7 g/10 min

@Load 3.80 kg,
Temperature 230 °C
2.7 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ASA S190
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 2.7 g/10 min

@Load 3.80 kg,
Temperature 230 °C
2.7 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ASA S750
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 2.7 g/10 min

@Load 3.80 kg,
Temperature 230 °C
2.7 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ASA S910
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 2.7 g/10 min

@Load 3.80 kg,
Temperature 230 °C
2.7 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers SE 3 HH
Description: High Heat ABSInformation provided by Diamond Polymers, Inc.