Total Finathene® CD 522 HDPE corrugated pipe resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Finathene® CD 522 HDPE corrugated pipe resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: corrugated pipe, storm and sanitary sewers, drainage systemsInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D 792
Environmental Stress Crack Resistance 100 hour
100 hour
ASTM D1697 cond. B 10% lgepal
600 hour
600 hour
ASTM D1697 cond. B 100% lgepal
Melt Flow 0.25 g/10 min

@Load 2.16 kg
0.25 g/10 min

@Load 4.76 lb
ASTM D 1238
High Load Melt Index 20 g/10 min

@Load 21.6 kg
20 g/10 min

@Load 47.6 lb
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 26.2 MPa
>= 3800 psi
ASTM D 638 type IV
Elongation at Break >= 600 %
>= 600 %
ASTM D 638 type IV
Flexural Modulus 1.31 GPa
190 ksi
ASTM D 790
Izod Impact, Notched 2.14 J/cm

@Thickness 3.17 mm
4.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Tensile Load, Notched Constant >= 24.0 hour
>= 24.0 hour
15% yield strength; ASTM D 5397
Thermal Properties Metric English Comments
Melting Point 128 °C
263 °F
ASTM D3417
Users viewing this material also viewed the following: