Tipco Tipcolene® ISL 10 BX1 - 10% Talc/Mineral Reinforced Polypropylene Homopolymer, High Flow, Stiffness & Impact Strength

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® ISL 10 BX1 - 10% Talc/Mineral Reinforced Polypropylene Homopolymer, High Flow, Stiffness & Impact Strength.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
10% Mineral Reinforced, High Stiffness, High Impact PP HomopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 75
75
Tensile Strength, Yield 24.5 MPa
3550 psi
ASTM D638
Elongation at Break >= 5.0 %
>= 5.0 %
ASTM D638
Flexural Yield Strength 31.0 MPa
4500 psi
ASTM D790
Flexural Modulus 1.96 GPa
284 ksi
ASTM D790
Izod Impact, Notched (ISO) 4.40 kJ/m²
2.09 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ASTM D648