Material Notes:
Data provided by the manufacturer, Abatron, Inc. Honey viscosity, light amber color. Best combination of high strength and versatility for Abatron "VR" Epoxies. Shelf life is 12+ months.Processing: 100/35 ratio. Pot life: 140 min. Peak exothermic temperature is 152°C (306°F). Cures at RT, but full mechanical, thermal, and corrosion properties are developed by heat cure or postcure.Applications: General purpose for casting, thick coating, bonding, embedding.Information provided by Abatron, Inc.
Physical Properties Metric English Comments
Viscosity 11000 - 14000 cP
11000 - 14000 cP
50-3
14000 - 20000 cP
14000 - 20000 cP
50-1
16000 cP

@Temperature 25.0 °C
16000 cP

@Temperature 77.0 °F
at 100/35 (50-3/50-1) pbw
Mechanical Properties Metric English Comments
Hardness, Rockwell M 80
80
Tensile Strength, Ultimate 57.22 MPa
8299 psi
Elongation at Break 3.9 %
3.9 %
Flexural Yield Strength 66.88 MPa
9700 psi
Flexural Modulus 2.41 GPa
350 ksi
Compressive Yield Strength 85.49 MPa
12400 psi
Compressive Modulus 2.55 GPa
370 ksi
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 - 110 °C
212 - 230 °F
Heat distortion temperature
105 °C
221 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity 1.22e+16 ohm-cm
1.22e+16 ohm-cm
Surface Resistance 5.50e+15 ohm
5.50e+15 ohm
Dielectric Constant 2.99

@Frequency 1e+6 Hz
2.99

@Frequency 1e+6 Hz
3.19

@Frequency 1000 Hz
3.19

@Frequency 1000 Hz
3.23

@Frequency 60 Hz
3.23

@Frequency 60 Hz
Dissipation Factor 0.0036

@Frequency 60 Hz
0.0036

@Frequency 60 Hz
0.0070

@Frequency 1000 Hz
0.0070

@Frequency 1000 Hz
0.019

@Frequency 1e+6 Hz
0.019

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Pot Life 140 min
140 min
500 g
Descriptive Properties Value Comments
Exotherm 152°C
Peak