Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.990 - 2.26 g/cc | 0.0358 - 0.0816 lb/in³ | Average value: 1.28 g/cc Grade Count:31 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Lucobit Lucofin® 1412 Polyolefin TPO Granules, Light Grey Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Lucobit Lucofin® 1461 Polyolefin TPO Granules, Ice Blue Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Lucobit Lucofin® 1452 Polyolefin TPO Granules, Blue Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
LyondellBasell Hifaxâ„¢ CA1110/2AC Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CA1110/2AC Black medium high melt flow, 1,200 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has a very good balance of processability, impact.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Lubricomp FX00617 PE LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Amer.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Lubricomp FX00617 PE (Asia Pacific) LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D792 |
Techmer ES Electrablend® HDPE 04001 LE BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ESD Protection and ConductiveAppearance: BlackProcessing Method: ExtrusionInformation provided by .. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | |
Solvay ANTAROX® AG/5 Surfactant Description: Modified alkanolamide Emulsifier for water based metal working fluids. Alternative to fatty alcohol ethoxylates and APE in metal working lubricants. Suitable for mineral paraffinic oil,.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | |
Solvay ANTAROX® FD 36 Surfactant Identification: FATTY ALCOHOL ALKOXYLATECAS: 68603 – 25 – 8Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Low foam wetting agent readily biodegradable, it.. |
|||
Density | 0.990 - 1.03 g/cc | 0.0358 - 0.0372 lb/in³ | AV15 |
Solvay Duraphos Octyl Acid Phosphate Surfactant Identification: DI(N-OCTYL) PHOSPHORIC ACID, N-OCTYL PHOSPHORIC ACID, PHOSPHORIC ACID CAS: 3115-39-7; 3991-73-9; 7664-38-2Solublility: Soluble in common organic solvents and slightly soluble in wate.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | |
Solvay IGEPAL® CA 210 Surfactant Description: Octyl phenol ethoxylate (1.5EO). Effective emulsifier for nonpolar solvents in solvent emulsion cleaners, pesticides, dry cleaning detergents and floor polishes. Nonionic dispersant and.. |
|||
Density | 0.990 - 1.01 g/cc @Temperature 20.0 °C |
0.0358 - 0.0365 lb/in³ @Temperature 68.0 °F |
|
Silikony Polskie Polsil E1 Silicone Emulsion POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. .. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOTUF MX00619 PP LNP* Thermotuf* MX00619 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Density | 0.990 - 1.03 g/cc | 0.0358 - 0.0372 lb/in³ | RP-17617 |
Solvay RHODOLINE® DF-988 Surfactant Description: Silicone free and mineral oil free defoamer for high gloss paints.Identification: DEFOAMERAvailable in: North AmericaApplications: RHODOLINE© DF-988 is a silicone-free, mineral oil-f.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D792 |
UBE UBESTA® 3030JI7 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: low migrationInformation provided by UBE. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D792 |
Tipco Tipcolene® FPW 10 PPC - 10% Wollastonite Reinforced Polypropylene Copolymer, High Impact Strength 10% Wollastonite Reinforced PP CopolymerApplications: Automotive & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D792 |
Tipco Tipcolene® UV 1022 - Polymeric-HALS (20% UV Stabilizer) Masterbatch in Polypropylene Homopolymer |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | |
ExxonMobil Mytex™ AS23K(W)-01 Talc filled compounded polypropylene produced for automotive interior applicationsInformation provided by ExxonMobil Chemical |
|||
Density | 0.990 g/cc @Temperature 15.6 °C |
0.0358 lb/in³ @Temperature 60.0 °F |
ASTM D4052 |
ExxonMobil Solvesso™ Aromatic 200 Aromatic Fluid Appearance: Clear/Transparent LiquidAvailability: North AmericaInformation provided by ExxonMobil |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D792 |
Diamond Polymers Softflex® SF 8900 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | |
Dow BETAFOAM™ 89120 Water/Amine catalyst BETAFOAM™ 89120 is a component used to make low density, all water blown rigid polyurethane foam.Information provided by Dow |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Eurotec® Tecolen® CP20 BK EC PPCP, conductive, black Information provided by Eurotec® |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D792 |
Aclo Accuguard Polypropylene HP0362V0CSL Homopolymer Flame Retardant Copper Stabilized |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | |
BASF Diisopropanol-p-toluidine Formula: C13H21NO2CAS: 38668-48-3Description: Diisopropanol-p-toluidine is a colorless to yellowish paste with and amine-like odor. This product is only sparingly soluble in water.Synonyms: DIIPT, .. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | |
BASF Lupragen® DMI 1,2-Dimethyl Imidazole Formula: C5H8N2CAS: 1739-81-0Description: 1,2-Dimethylimidazole is a colorless to yellowish solid with an amine-like odor. Synonyms: DMI, 1,2-Dimethyl-1H-imidazolApplications: It is used as a Cataly.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | |
A. Schulman ComAlloy Comtuf® 103 Polypropylene, Glass Reinforced, Chemically Coupled, Impact Modified Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOTUF MX00619 PP (Asia Pacific) LNP* Thermotuf* MX00619 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | DIN 53479 |
Polyram RamOfin PPC300S4BK10 Polypropylene, 20% Glass beads 20% glass beads reinforced polypropylene copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | |
Solvay RHODASURF® DA-630 E Surfactant Description: Rhodapon® LS-92/RN is high purity, dust free anioinic surfactant in a needle form. Free flowing and easily dispersed in water. Excellent foaming and detergent properties.Identification.. |