Dow BETAMATE™ XW 1044-3 Epoxy

Category Polymer , Thermoset , Epoxy
Manufacturer Dow Chemical
Trade Name BETAMATE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow BETAMATE™ XW 1044-3 Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BETAMATE™ XW 1044-3 is a one component, epoxy based adhesive especially developed for the body shop. The adhesive can be applied by robot systems and it shows high adhesion to metal and non-metal surfaces.Information provided by Dow
Physical Properties Metric English Comments
Density 1.31 - 1.37 g/cc
0.0473 - 0.0495 lb/in³
Solids Content >= 99 %
>= 99 %
Viscosity 650000 cP

@Shear Rate 1.00 1/s,
Temperature 40.0 °C
650000 cP

@Shear Rate 1.00 1/s,
Temperature 104 °F
cone/plate
4.00e+6 cP

@Shear Rate 1.00 1/s,
Temperature 23.0 °C
4.00e+6 cP

@Shear Rate 1.00 1/s,
Temperature 73.4 °F
cone/plate
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 35.0 MPa
5080 psi
ISO 527-1
Elongation at Break 2.3 %
2.3 %
ISO 527-1
Modulus of Elasticity 2.90 GPa
421 ksi
ISO 527-1
Adhesive Bond Strength 16.9 MPa

@Thickness 0.750 mm
2450 psi

@Thickness 0.0295 in
Lap Shear (25 x 10 x 0.2 mm) (CRS St 1203); EN 1465
23.7 MPa

@Thickness 1.50 mm
3440 psi

@Thickness 0.0591 in
Lap Shear (25 x 10 x 0.2 mm) (CRS St 1203); EN 1465
Peel Strength 3.70 kN/m
21.1 pli
T-Peel (CRS St 1203, 0.5mm)
8.00 kN/m
45.6 pli
Impact Peel
Thermal Properties Metric English Comments
Flash Point >= 150 °C
>= 302 °F
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 180 °C
0.500 hour

@Temperature 356 °F