Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
RheTech Products CC20P200-00 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Natural
Applications: Electrical housingsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
RheTech Products FRP256-00 Polypropylene Copolymer, Flame Retardant, Natural
Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
RheTech Products FRp256-01 Polypropylene Copolymer, Flame Retardant, Black
Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
RheTech Products FT1001-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Facias, claddings, and rocker panelsBodyside moldingsStep pads and bumper componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
RheTech Products FT1001-177UV Thermoplastic Polyolefin, Non-UV Stabilized, HS5 Medium Dark Neutral
Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
RheTech Products FT1001-74 Thermoplastic Polyolefin, Non-UV Stabilized, DX9 Black
Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
RheTech Products FT1002-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
RheTech Products FT1003-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step and hitch padsInterior component and trimA/B pillarsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
RheTech Products FT2600-00UV Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Interior trimSplash shieldScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
RheTech Products FT2600-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Interior trimSplash shieldsStep pads and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
RheTech Products FT2600-677UV Thermoplastic Polyolefin, UV Stabilized, 0848 Black
Applications: Exterior trimStep pads and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
RheTech Products FT2700-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
RheTech Products FT2700-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
RheTech Products P252-00 Polypropylene Copolymer, Natural
Applications: Interior trimUnderhood componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
RheTech Products T10P250-00 10% Talc Reinforced Polypropylene Copolymer, Natural
Applications: Fan shroudsCenter consolesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
RheTech Products T10P250-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black
Applications: Wire troughFan shroudsElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
RheTech Products T28P100-01EG 28% Talc Reinforced Polypropylene, Black, Extrusion Grade
Applications: Window trimConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
Celanese Vandar® 9056 Thermoplastic Polyester Alloy
Unreinforced; highest flexibilityInformation provided by Celanese Corporation.
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
Celanese Vandar® 9116 Thermoplastic Polyester Alloy
Unreinforced; highest flexibility (SRS grade)Information provided by Celanese Corporation.
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
Tipco Tipcolene® ISL 10 BX1 - 10% Talc/Mineral Reinforced Polypropylene Homopolymer, High Flow, Stiffness & Impact Strength
10% Mineral Reinforced, High Stiffness, High Impact PP HomopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., Indi..
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
PolyOne Synprene® RT-3840MS Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerTransparentUV StabilizedApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation..
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
RheTech Products CC20P200-01 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Black
Applications: Electrical housingsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
PolyOne Synprene® IT 62-001 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Over-Molding GradeNaturalTransparentUV StabilizedApplications:Multi-PurposeProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
Plastcom SLOVALEN PC 92 T 40 PP, 40% mineral filling
FeaturesModified homopolymer and copolymer PP for injection moulding with the contenct of 40% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C..