Tipco Tipcolene® FPC 20 PPC - 20% Calcium Carbonate Reinforced Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® FPC 20 PPC - 20% Calcium Carbonate Reinforced Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% Calcium Carbonate Filled PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Melt Flow 7.0 g/10 min
7.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.5 MPa
3550 psi
ASTM D638
Elongation at Break >= 100 %
>= 100 %
ASTM D638
Flexural Yield Strength 34.0 MPa
4930 psi
ASTM D790
Flexural Modulus 1.57 GPa
228 ksi
ASTM D790
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
ASTM D256