Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Yield Strength = 4930 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 34.0 MPa
4930 psi
ISO METHOD 176
NYCOA 2046 Copolymer Nylon 6/69
extrusion, moderate melt viscosity, high strength mono.Information provided by NYCOA, Inc.
Flexural Yield Strength 34.0 MPa
4930 psi
ASTM D790
Ineos Nova 731G High Impact Polystyrene  (discontinued **)
Balance of stiffness and toughness, High impact, USP Class VIApplications: Razor components, Personal care, Consumer goodsIn addition, exposure to gamma radiation in the 2.02-6.06 megarad range ahs ..
Flexural Yield Strength 34.0 - 60.0 MPa
4930 - 8700 psi
Average value: 51.1 MPa Grade Count:9
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m..
Flexural Yield Strength 34.0 MPa
4930 psi
ASTM D790
PolyOne Stat-Tech™ AS-15CP/000 ABS - 15% Carbon Powder  (discontinued **)
Data provided by PolyOne.
Flexural Yield Strength 34.0 MPa
4930 psi
ASTM D790
PolyOne Lubri-Tech™ ATH-000/05M Acetal Homopolymer - 5% MoS2  (discontinued **)
Data provided by PolyOne.
Flexural Yield Strength 34.0 MPa
4930 psi
Test specimens were injection molded by ASTM D1897; ASTM D790
Chevron Phillips K-Resin® KR99HG Styrene-Butadiene Copolymer, Injection Molding Grade  (discontinued **)
Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed by injection molding. Molded parts provide excellent part detail on fast production cycles. Molded parts have excellent c..
Flexural Yield Strength 34.0 MPa
4930 psi
At 3.5% strain
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin
Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a..
Flexural Yield Strength 34.0 MPa
4930 psi
ASTM D790
Ineos Nova 5511 High Impact Polystyrene
Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Industrial productsProperties were determined on injection molded specimens at 23°C..
Flexural Yield Strength 34.0 MPa
4930 psi
ASTM D790
Ineos Nova 6200 Super High Impact Polystyrene
Good toughness, Deep draw, Easy processing using all conventional methodsApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined..
Flexural Yield Strength 34.0 MPa
4930 psi
ASTM D790
Ineos Nova 6201 Super High Impact Polystyrene
Good toughness, Deep draw, Easy processing using all conventional methodsApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined..
Flexural Yield Strength 34.0 MPa
4930 psi
ASTM D790
Tipco Tipcolene® CR 7228 - 30% Talc/Mineral Reinforced Polypropylene Copolymer
30% Mineral Reinforced PP CopolymerApplications: Automotive DashboardsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Flexural Yield Strength 34.0 MPa
4930 psi
ASTM D790
Tipco Tipcolene® FPC 20 PPC - 20% Calcium Carbonate Reinforced Polypropylene Copolymer
20% Calcium Carbonate Filled PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Flexural Yield Strength 34.0 MPa
4930 psi
ASTM D790
Tipco Tipcolene® ISRH 35 NF - 20% Talc/Mineral Reinforced Polypropylene Homopolymer, High Flow
20% Mineral Reinforced, PP HomopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Flexural Yield Strength 34.0 MPa
4930 psi
ASTM D790
Tipco Tipcolene® PPH-OIT - Unfilled Polypropylene Homopolymer Compound with Copper Inhibitor (Metal Deactivator)
PP Homopolymer with Copper Inhibitor (Metal De-activator)Applications: Automotives & ElectricalProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Flexural Yield Strength 34.0 MPa
4930 psi
ASTM D790
Chevron Phillips K-Resin® KR03 Styrene-Butadiene Copolymer, Sheet Grade
Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give excellent part detail on fast production cycles. It can be t..
Flexural Yield Strength 34.0 MPa
4930 psi
ASTM D790
Chevron Phillips K-Resin® KR03NW Styrene-Butadiene Copolymer, Sheet Grade
Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR03 to facilitate printing.Customer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give ..
Flexural Yield Strength 34.0 MPa
4930 psi
ASTM D790
Chevron Phillips K-Resin® KR05 Styrene-Butadiene Copolymer, Sheet and Blow Mold Grade
Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed on blow molding or extrusion and thermoforming equipment. Finished products have excellent clarity, good toughness, good s..
Flexural Yield Strength 34.0 MPa
4930 psi
ASTM D790
Chevron Phillips K-Resin® KR05NW Styrene-Butadiene Copolymer, Sheet and Blow Mold Grade
Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR05 to facilitate printing.Customer Benefits: This SBC is easily processed on blow molding or extrusion and thermoforming equipment. Fin..
Flexural Yield Strength 34.0 MPa
4930 psi
ASTM D790
Covestro Baydur® SFR-243 Polyurethane Composite RRIM Foam, MDI-based 2-Component Liquid System
0.25 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – C..
Flexural Yield Strength 34.0 MPa
4930 psi
ASTM D790
Ineos Nova 6260 Super High Impact Polystyrene  (discontinued **)
Good toughness, Deep draw, Easy processing using all conventional methodsApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined..
Flexural Yield Strength 34.0 MPa
4930 psi
ASTM D790
Chevron Phillips K-Resin® BK11 Styrene-Butadiene Copolymer, Injection Molding Grade  (discontinued **)
Styrene-Butadiene CopolymerCustomer Benefits: BK11 is an SBC consisting of KR03 grade with a mold release added of easier processing. BK11 molded parts give excellent detail on fast production cycl..
Flexural Yield Strength 34.0 MPa
4930 psi
At 3.5% strain
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin
Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a..
Copyright © lookpolymers.com All Rights Reserved