Material Notes:
DescriptionSchulaflex SF302 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and ESCR tests were performed on compression molded samples. ApplicationSF302 is ideally suited for products requiring a soft feel.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ASTM D792
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
F50; ASTM D1693
Melt Index of Compound 9.0 g/10 min
9.0 g/10 min
2.16/190; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 38
38
15 sec delay; ASTM D2240
Tensile Strength, Yield 6.89 MPa
1000 psi
2 in/min; ASTM D638
Elongation at Break 820 %
820 %
2 in/min; ASTM D638
Users viewing this material also viewed the following: