Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 11.7 MPa | 1700 psi | 2 in/min; ASTM D638 |
Polimeros Mexicanos Rotolene® ECO-BLACK Linear Medium Density Polyethylene MDPE Copolymer with UV8 stabilizer, available as black powder.Recommended for rotomolding. Used for manufacture of septic tanks and garbage bins. Recommended for use in combination with ROTOFOAM B.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | Cured |
Resin Technology Group UV-422 Flexible, UV Curing Sealant UV 422 is a semi-flexible, UV curing adhesive that can be used in a wide variety of potting, sealing, tacking and bonding applications. High strength bonds are formed to PVC and polycarbonate substr.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible D8500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C8000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D638 |
LyondellBasell Microthene® F FE53200 Ethylene Vinyl Acetate Copolymer General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D638 |
LyondellBasell Petrothene® NA951080 Low Density Polyethylene ApplicationsPETROTHENE NA 951-080 is designed for use as a base resin for compounding material including gas-injected or chemically expanded insulation. NA 951-080 is a natural, low density, medium.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D1414 |
Greene Tweed CHEMRAZ® 543 Perfluoroelastomer Chemraz® 543 is recommended for a wide variety of semiconductor equipment dry processing applications where seal reliability with minimal contamination is required. It offers excellent performan.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D412 |
ITW Devcon Flexane® Rubber Repair / Castable Urethane Belt Repair Kit, Black Information provided by ITW Devcon |
|||
Tensile Strength at Break | >= 11.7 MPa | >= 1700 psi | |
Sibur 1045-12 Compound 948 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | 500 mm/min; GOST 11262 |
Sibur 15803-020 Low Density Polyethylene For production of films and film articles, including thermoset films, thin films, food contact grade films
(including tight packing), general-purpose films, and bags. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D638 |
Teknor Apex APEX® 3701-65NT Polyvinyl Chloride, Flexible Features: Non-DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D412 |
Teknor Apex Monprene® MP-1500SC Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D638 |
Teknor Apex APEX® 1009 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D638 |
Teknor Apex APEX® 3800-65 Polyvinyl Chloride, Flexible Features: DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor .. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D412 |
Teknor Apex Monprene® MP-1855J Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D412 |
Teknor Apex Monprene® MP-3955B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D412 |
Teknor Apex Telcar® TL-1268A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D412 |
Teknor Apex Telcar® TL-1434A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D412 |
Teknor Apex Telcar® TL-4145 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D412 |
Teknor Apex Telcar® TL-83-F912-E-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D412 |
Teknor Apex Telcar® TL-83-F912-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D638 |
ExxonMobil LDPE LD 100BW Low Density Polyethylene Resin (European Grade) Product Description: LD 100BW is a LDPE containing low antioxidants suitable for the production of LV and MV crosslinked insulation using the 1-step or 2-step silane technology. Through in-house com.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 291-75B150 Thermoplastic Vulcanizate Product Description: A colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PC, ABS, PC/ABS, ASA and PMMA for app.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D638 |
ExxonMobil Paxon™ BA7794 Sheet Extrusion and Blow Molding Resin
(discontinued **) BA7794 is a 25% talc-filled, high molecular weight, high density polyethylene. This color match-able material has been specifically developed as a cost effective resin for applications which requir.. |
|||
Tensile Strength at Break | 11.7 - 15.2 MPa | 1700 - 2200 psi | |
ITW Plexus Plexus™ MA925 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, long open time.Information provided by Illinois Tool Works. |