Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
PolyOne Versaflex™ OM 6258-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 6258-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
Ineos Nova 474 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Custom ColorsApplications: Injection molding, Alternative to engineering resinsPerformance grades of polystyrene are engineered to have specific properties. These products can be custom colored. N.. |
|||
Rear Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® PP-60/V2 Polypropylene Homopolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
Ineos Nova Styrosun® 3600 Weather Resistant High Impact Styrenic Polymer Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP 1141 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-1274G Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-1277B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-1473F Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-1580B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-1662-L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-1702B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-1775D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-1797 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-1848 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-2242 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-2290 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-2634A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-2760BR Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-2790 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-2850E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-2955 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 3170 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3170 can be processed by blow molding, injection molding or.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 4165 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4165 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 4390 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4390 is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set .. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 3140 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3140 can be processed by injection molding or extrusion for appl.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 4139D Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4139D is a high hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 4339D Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4339D is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set .. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-2870E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 3439DN Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 4149D Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4149D is a high hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |