Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 11.7 MPa | 1700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne FireCon™ CPE 30-11 REV 2 Polyethylene, Chlorinated (CPE) CPE-30-11 REV 2 is a heavy duty thermoplastic jacket for power and control cables. It is suitable for VW1 and tray fire rated applications. CPE-30-11 REV 2 offers high tensile and superior fluid res.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne FireCon™ CPE 30-11 RoHS BLACK Polyethylene, Chlorinated (CPE) CPE-30-11 RoHS BLACK is a heavy duty thermoplastic jacket for power and control cables. It is suitable for VW1 and tray fire rated applications. CPE-30-11 RoHS BLACK offers high tensile and superior.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible D8500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C8000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D638 |
LyondellBasell Microthene® F FE53200 Ethylene Vinyl Acetate Copolymer General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D638 |
LyondellBasell Microthene® G MU76300 Ethylene Vinyl Acetate Copolymer General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D412 |
ITW Devcon Flexane® Rubber Repair / Castable Urethane Belt Repair Kit, Black Information provided by ITW Devcon |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | |
Shin-Etsu Silicones FE-361U Fluorosilicone Elastomer ShinEtsu FE361 U is one of a series of high tensile, high tear fluorosilicone compounds. It is designed to process well in molding applications. It can be blended with other members of the series fo.. |
|||
Tensile Strength at Break | >= 11.7 MPa | >= 1700 psi | |
Sibur O-55 Compound 1182 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D412 |
Teknor Apex Monprene® MP-1500SC Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D412 |
Teknor Apex Monprene® MP-2242 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D638 |
Teknor Apex APEX® 1003 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D638 |
Teknor Apex APEX® 1004 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D638 |
Teknor Apex APEX® 3800-65 Polyvinyl Chloride, Flexible Features: DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor .. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D412 |
Teknor Apex Monprene® MP-3955B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D412 |
Teknor Apex Telcar® TL-1268A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D412 |
Teknor Apex Telcar® TL-1434A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D412 |
Teknor Apex Telcar® TL-83-F912-E-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D412 |
Teknor Apex Telcar® TL-83-F912-G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D412 |
Teknor Apex Telcar® TL-83-F912-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D412 |
Teknor Apex Telcar® TL-8732R Thermoplastic Elastomer Notes: RoHS Compliant Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstri.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D638 |
ExxonMobil LDPE LD 100BW Low Density Polyethylene Resin (European Grade) Product Description: LD 100BW is a LDPE containing low antioxidants suitable for the production of LV and MV crosslinked insulation using the 1-step or 2-step silane technology. Through in-house com.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D638 |
ExxonMobil LDPE LD 101BA Wire & Cable Low Density Polyethylene Resin Product Description: LD 101BA Wire & Cable is anon-stabilized LDPE, designed for the production of Medium/High Voltage insulation using the direct peroxide addition. For cleanliness reasons, the mat.. |
|||
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D638 |
ExxonMobil Escorene® LD 728.61 Molding, extrusion and compounding resin Escorene Ultra LD 728.61 is a high vinyl acetate copolymer with low melting temperature and excellent strength properties and toughness.Availability: Latin America, North America and South America A.. |
|||
Tensile Strength at Break | 11.7 - 15.2 MPa | 1700 - 2200 psi | |
ITW Plexus Plexus™ MA925 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, long open time.Information provided by Illinois Tool Works. |