Material Notes:
Features: Good Thermal Stability; Recyclable Material; Good Weather Resistance; Ultra High Molecular Weight Uses: Medical/Healthcare Applications; Pump Parts; Tubing Agency Ratings: FDA Unspecified Rating Forms: Pellets Processing Method: Extrusion; Injection MoldingInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
15 seconds; ASTM D2240
Tensile Strength at Break 16.7 MPa
2420 psi
ASTM D638
Tensile Stress 8.41 MPa

@Strain 100 %
1220 psi

@Strain 100 %
ASTM D638
Elongation at Break 370 %
370 %
ASTM D638
Tear Strength 46.5 kN/m
265 pli
Die C; ASTM D624
Compression Set 20 %

@Temperature 22.8 °C,
Time 79200 sec
20 %

@Temperature 73.0 °F,
Time 22.0 hour
ASTM D395
56 %

@Temperature 70.0 °C,
Time 79200 sec
56 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395
60 %

@Temperature 100 °C,
Time 79200 sec
60 %

@Temperature 212 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -40.0 °C
-40.0 °F
ASTM D746
Processing Properties Metric English Comments
Rear Barrel Temperature 182 - 199 °C
360 - 390 °F
Middle Barrel Temperature 182 - 199 °C
360 - 390 °F
Front Barrel Temperature 182 - 199 °C
360 - 390 °F
Mold Temperature 23.9 - 51.7 °C
75.0 - 125 °F
Back Pressure 0.345 - 1.03 MPa
50.0 - 150 psi
Descriptive Properties Value Comments
Screw Compression Ratio 2:1 - 3:1
Screw L/D Ratio 20:1 - 24:1
Suggested Regrind, max 20