Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
PolyOne Versaflex™ HC MT555 Thermoplastic Elastomer (TPE) Versaflex™ HC MT555 is an easy processing material designed for applications where FDA compliance and medical testing is required. - Excellent Colorability - Soft TouchRear: 340 - 360F Center: 380 .. |
|||
Middle Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
PolyOne Versaflex™ OM 1060X-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 1060X-1 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, ABS, PC/ABSColor conce.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
PolyOne Versaflex™ OM 9-802CL Thermoplastic Elastomer (TPE) Versaflex™ OM 9-802CL is a clear, soft touch TPE designed to bond to the following thermoplastics: PC, ABS, PC/ABS and copolyester. New Product. Commercial specifications have not been established... |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
PolyOne Versaflex™ VDT 4132 Thermoplastic Elastomer (TPE) Versaflex™ VDT 4132 is designed to create vibration damping. - Excellent Vibration DampingRear = 350-370F Middle = 375-400F Front = 375-400F Nozzle = 365-380F Screw speed = 100-500rpmPurge thorough.. |
|||
Middle Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
PolyOne Versollan™ OM 1255NX-9 Thermoplastic Elastomer (TPE) Versollan™ OM 1255NX-9 is a performance TPU alloy designed for thin wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Improved Grip with Matte, Rubbery Finish - Superior Adhesi.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | |
Oxford Polymers C-Acetal -30GF-Natural Acetal Copolymer, 30% Glass Fiber Reinforced Product Description: Glass Fiber (30% Reinforced), Co-polymer Acetal, Injection Molding Grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Glass FiberSpecial Characteristic.. |
|||
Middle Barrel Temperature | 182 - 193 °C | 360 - 380 °F | |
Polymer Resources AC-G10 Acetal Copolymer, 10% Glass Reinforced Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Teknor Apex Flexalloy® 9100-75 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Middle Barrel Temperature | 182 - 216 °C | 360 - 421 °F | |
Styrolution NAS® 90 High Performance Styrenic NAS® 90 has sparkling clarity, improved toughness, and good scratch resistance. This easily processed copolymer blends well with clear impact modifiers. It meets USP XXIII Spec. of Class VI Pla.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3145D Thermoplastic Elastomer A high hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3145D can be processed by injection blow molding, molding or .. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3440 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3460 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3490N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4190 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4190 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4370 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4370 is a flame retardant, soft hardness grade exhibiting exceptional chemical resistance, compression set.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4390 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4390 is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set .. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4449D Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4449D is a high hardness grade possessing exceptional tensile strength, superior compression.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4455 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4455 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Middle Barrel Temperature | 182 °C | 360 °F | |
ExxonMobil Santoprene® 171-64 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Middle Barrel Temperature | 182 °C | 360 °F | |
ExxonMobil Santoprene® 201-64 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Middle Barrel Temperature | 182 °C | 360 °F | |
ExxonMobil Santoprene® 271-55 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Middle Barrel Temperature | 182 °C | 360 °F | |
ExxonMobil Santoprene® 271-64 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3480 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3490 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Middle Barrel Temperature | 182 °C | 360 °F | |
ExxonMobil Santoprene® 171-55 Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3150 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3150 can be processed by injection molding or extrusion for appl.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3180 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3180 can be processed by blow molding injection molding or ex.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3439DN Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4149D Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4149D is a high hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Middle Barrel Temperature | 182 °C | 360 °F | |
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer Product Description: A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for.. |