Material Notes:
Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Melt Flow 20 g/10 min

@Load 10.0 kg,
Temperature 220 °C
20 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Elongation at Break 3.1 %
3.1 %
ASTM D638
Flexural Strength 71.0 MPa
10300 psi
ASTM D790
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
1.00 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
0.854 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
1.60 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
2.67 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
5.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 91.1 °C
196 °F
Unannealed; ASTM D648
104 °C
219 °F
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 77.8 °C
172 °F
Unannealed; ASTM D648
98.9 °C
210 °F
Annealed; ASTM D648
Users viewing this material also viewed the following: