Polymer Property : Izod Impact, Notched = 1.60 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.854 J/cm

@Temperature 22.8 °C
1.60 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PPX-FRG10 Modified-PPO, V-1 Flame Retardant, 10% Glass Reinforced
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 10% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu..
Izod Impact, Notched 0.854 J/cm

@Temperature 0.000 °C
1.60 ft-lb/in

@Temperature 32.0 °F
ASTM D256
Ineos L06Z-00 Polypropylene Impact Copolymer
This is a medium MFR impact copolymer polypropylene made for injection molded caps and closures applications. It offers a good balance of stiffness to impact resistance as compared to other impact ..
Izod Impact, Notched 0.854 J/cm

@Temperature -20.0 °C
1.60 ft-lb/in

@Temperature -4.00 °F
ASTM D256
Ineos N01G-02 Polypropylene Impact Copolymer
N01G-02 is a low melt flow rate polypropylene impact copolymer designed for blow molding, extrusion, and compounding applications. The grade benefits from a very high impact resistance at room and l..
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
1.60 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES HiFill FR® PA6/6 GF30 FR-N 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame Retardant and Halogen FreeInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm,
Temperature -17.8 °C
1.60 ft-lb/in

@Thickness 0.125 in,
Temperature 0.000 °F
ASTM D256
Techmer ES Plastiblend® ABS 8007
Availability: North AmericaForms: PelletsFeatures: General Purpose and High FlowInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
1.60 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8009 FR
Availability: North AmericaForms: PelletsFeatures: Flame Retardant and High Heat ResistanceInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.853 J/cm

@Thickness 3.17 mm
1.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® GP-5300G PBT, Glass Filled
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.853 J/cm

@Thickness 6.35 mm
1.60 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® GR-4010 ABS, 10% Glass Filled
Material with 10% GF reinforcement with high stiffness that can be used in refrigerator vegetable boxesInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 0.853 J/cm

@Thickness 3.17 mm
1.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® GP-5300G PBT, Glass Filled
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.853 J/cm

@Thickness 6.35 mm
1.60 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® GR-4010 ABS, 10% Glass Filled
Material with 10% GF reinforcement with high stiffness that can be used in refrigerator vegetable boxesInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 0.854 J/cm

@Temperature 23.0 °C
1.60 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Formosa Plastics Formolene® 2315N Impact Copolymer Polypropylene
Impact Copolymer for Injection Molding Applications Requiring Stiffness Formolene® 2315N is a high flexural modulus copolymer of polypropylene designed and formulated for injection-molded applicati..
Izod Impact, Notched 0.854 J/cm

@Temperature -30.0 °C
1.60 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Formosa Plastics Formolene® 6600A Impact Copolymer Polypropylene
Impact Copolymer for Extrusion and Compounding Applications (Fractional Melt Flow) Formolene® 6600A is a high impact copolymer with an excellent balance of toughness and stiffness. It is suitable f..
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.60 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Diamond Polymers Centrex® 810 Injection Molding Grade
Centrex 810 resin is a soft-flow, high-gloss, and medium-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and ..
Izod Impact, Notched 0.854 J/cm

@Temperature 0.000 °C
1.60 ft-lb/in

@Temperature 32.0 °F
ASTM D256A
Dow C702-20NA Polypropylene Impact Copolymer Resin
OverviewHigh impact performanceContains a nucleating additiveContains an antistatic additiveComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW C702-20NA Polypropylene Resin is intended f..
Izod Impact, Notched 0.854 J/cm

@Temperature 23.0 °C
1.60 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Dow C759-21NA Polypropylene Impact Copolymer Resin
DOW C759-21NA Polypropylene Resin is an impact copolymer designed for injection molding with high stiffness, good impact resistance, and good antistatic properties. Key applications include foldabl..
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm,
Temperature -18.0 °C
1.60 ft-lb/in

@Thickness 0.125 in,
Temperature -0.400 °F
0.5 x 0.125 in.; ASTM D256
Americas Styrenics STYRON™ 487 High-Impact Polystyrene Resin
STYRON™ 487 is a high-impact polystyrene with an excellent balance of flow, toughness, stiffness and heat resistance. It has excellent deep draw characteristics and is appropriate for extrusion ap..
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
1.60 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 922 NAT
Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
1.60 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D-256
Axiall 9129J Rigid PVC, Extrusion
Georgia Gulf 9129J is designed for use in extruded price tag holders. The compound contains an ultraviolet light stabilizer which retards color change.Information provided by Georgia GulfGeorgia Gu..
Izod Impact, Notched 0.854 J/cm

@Temperature -30.0 °C
1.60 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Formosa Plastics Formolene® 2620A Impact Copolymer Polypropylene
Impact Copolymer for Compounding and Injection Molded Applications Formolene® 2620A is a high impact copolymer of polypropylene designed for applications such as automotive compounds and lawn & gar..