Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.534 J/cm @Temperature 22.8 °C |
1.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature -30.0 °C |
1.00 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature -30.0 °C |
1.00 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-G20 Modified-PPO, 20% Glass Reinforced Modified-Polyphenylene Oxide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature -30.0 °C |
1.00 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-G30 Modified-PPO, 30% Glass Reinforced Modified-Polyphenylene Oxide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature -40.0 °C |
1.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources ABS-GP-HH General Purpose ABS, High Heat General Purpose Acrylonitrile Butadiene Styrene, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature -20.0 °C |
1.00 ft-lb/in @Temperature -4.00 °F |
1/8'' notched bar; ASTM D256 |
Ineos N05U-00 Polypropylene Impact Copolymer This is an extrusion-grade nucleated impact copolymer polypropylene resin designed for fiber optic buffer tube applications in the protection of glass fibers. It also has an excellent impact/stiffn.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 IM 408 L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc... |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -28.9 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -20.0 °F |
ASTM D256 |
Techmer ES HiFill® PP CO GF30 CC 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES HiFill® PP GF/M30 CC BK 30% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 30% Filler by WeightFeatures: Chemically Coupled and CopolymerAppearance: BlackInformation provided by TP Composites, In.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Luriblend® PA4/6 TL15 HS Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized, Low Friction, Good Wear Resistance and LubricatedInformation provided by TP Com.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS GN005 Availability: North AmericaForms: PelletsFeatures: General PurposeAppearance: GreenInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS NAT Availability: North AmericaForms: PelletsFeatures: General PurposeAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS/PA 1700 B1 Availability: North AmericaForms: PelletsAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 IM 408 HS L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -28.9 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -20.0 °F |
ASTM D256 |
Techmer ES HiFill® PP CO GF20 CC 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Luriblend® ABS TL2 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature 0.000 °C |
1.00 ft-lb/in @Temperature 32.0 °F |
ASTM D256A |
Formosa Plastics Formolene® 2306N Impact Copolymer Polypropylene Impact Copolymer for Compression and Injection Molded Caps and Closures Formolene® 2306N is a polypropylene copolymer formulated for compression and injection molded cap applications. It was create.. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature -50.0 °C |
1.00 ft-lb/in @Temperature -58.0 °F |
ASTM D256 |
Dow AFFINITY™ SM 1300G Polyolefin Plastomer (POP) AFFINITY™ SM 1300G is an ethylene alpha-olefin resin for Injection Molding is produced via INSITE™ Technology from Dow Plastics. The resin offers excellent performance in durable injection molded.. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature 23.0 °C |
1.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Dow C705-44NA Polypropylene Impact Copolymer Resin DOW C705-44NA Polypropylene Resin is a high melt flow rate impact copolymer that combines superior stiffness and good impact resistance. The product is intended for use in injection molding applica.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall CL-6380, CL-6380J Rigid PVC, Molding Georgia Gulf CL-6380 & CL-6380J are clear fittings compounds with cell class 12454(Type 1, Grade 1). These compounds are ideally suited for swimming pools, spas, and numerous applications where vis.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.00 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall CL-7053 Rigid PVC, Molding Georgia Gulf CL-7053 is a clear, high flow vinyl compound designed for a variety of end-use molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -20.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
ASTM D-256 |
Axiall HH-2000 Rigid PVC, Molding Georgia Gulf HH-2000 is a high heat/high flow injection molding grade PVC alloy with a price/performance niche between high flow vinyl and utility engineering thermoplastics. It combines excellent .. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -20.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
ASTM D-256 |
Axiall UV-6680 Rigid PVC, Molding Georgia Gulf UV-6680 is a weatherable, high flow injection molding compound, specially formulated for outdoor UV exposure. This compound was designed to be used in various accessory parts, such as .. |
|||
Izod Impact, Notched | >= 0.534 J/cm @Temperature -30.0 °C |
>= 1.00 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Buckeye Polymers BP FLEX D6520 T BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -20.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
ASTM D-256 |
Axiall UV-7160 Rigid PVC, Molding Georgia Gulf UV-7160 is a rigid vinyl injection molding compound characterized by excellent flow, toughness, heat stability, color hold and surface appearance. This combination of outstanding attri.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8008 Availability: North AmericaForms: PelletsFeatures: General Purpose Appearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -20.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
ASTM D-256 |
Axiall 6509 Rigid PVC, Molding Georgia Gulf 6509 is a non-regulated, high flow, injection molding compound that has been specifically designed for outdoor applications that require an added degree of static resistance.Information.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Luriblend® ABS SLX2 MB Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: General Purpose and LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Luriblend® ABS TL10 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |