Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.534 J/cm @Temperature -40.0 °C |
1.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources ABS-GP1 General Purpose ABS General Purpose Acrylonitrile Butadiene StyreneFeatures: • Medium Impact ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature -40.0 °C |
1.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature 22.8 °C |
1.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature -30.0 °C |
1.00 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature -30.0 °C |
1.00 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-G10HF Modified-PPO, 10% Glass Reinforced, High Flow Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature -30.0 °C |
1.00 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-G20 Modified-PPO, 20% Glass Reinforced Modified-Polyphenylene Oxide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -28.9 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -20.0 °F |
ASTM D256 |
Techmer ES HiFill® PP CO GF30 CC 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES HiFill® PP GF/M30 CC BK 30% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 30% Filler by WeightFeatures: Chemically Coupled and CopolymerAppearance: BlackInformation provided by TP Composites, In.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Luriblend® PA4/6 HS TL15 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized and LubricatedUL File Number: E157318Information provided by TP Composites, Inc... |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS GN005 Availability: North AmericaForms: PelletsFeatures: General PurposeAppearance: GreenInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS NAT Availability: North AmericaForms: PelletsFeatures: General PurposeAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 IM 408 HS L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Electrablend® PA6/6 03005 CF Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Electrically Conductive, Impact.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Luriblend® ABS SL2 Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: General Purpose and LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Luriblend® ABS TL2 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 92RK Availability: North AmericaForms: PelletsFeatures: General PurposeProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS LE BK Availability: North AmericaForms: PelletsFeatures: Low ExtractablesAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Diamond Polymers Centrex® 810 Injection Molding Grade Centrex 810 resin is a soft-flow, high-gloss, and medium-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and .. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature 23.0 °C |
1.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Dow C705-44NA Polypropylene Impact Copolymer Resin DOW C705-44NA Polypropylene Resin is a high melt flow rate impact copolymer that combines superior stiffness and good impact resistance. The product is intended for use in injection molding applica.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -20.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
ASTM D-256 |
Axiall HH-2000 Rigid PVC, Molding Georgia Gulf HH-2000 is a high heat/high flow injection molding grade PVC alloy with a price/performance niche between high flow vinyl and utility engineering thermoplastics. It combines excellent .. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -20.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
ASTM D-256 |
Axiall MP-6585 Rigid PVC, Molding Georgia Gulf MP-6585 is an electrical grade rigid vinyl injection molding compound processing good strength, stiffness, toughness, and flow. In addition, it has excellent processing stability and s.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -20.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
ASTM D-256 |
Axiall UV-7160 Rigid PVC, Molding Georgia Gulf UV-7160 is a rigid vinyl injection molding compound characterized by excellent flow, toughness, heat stability, color hold and surface appearance. This combination of outstanding attri.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8008 Availability: North AmericaForms: PelletsFeatures: General Purpose Appearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 922 NAT Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -20.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
ASTM D-256 |
Axiall 6509 Rigid PVC, Molding Georgia Gulf 6509 is a non-regulated, high flow, injection molding compound that has been specifically designed for outdoor applications that require an added degree of static resistance.Information.. |
|||
Izod Impact, Notched | >= 0.534 J/cm @Temperature -30.0 °C |
>= 1.00 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Buckeye Polymers BP FLEX D5518 R 848 Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Luriblend® ABS SLX2 MB Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: General Purpose and LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Luriblend® ABS TL10 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Luriblend® ABS X MB Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: General Purpose and LubricatedInformation provided by TP Composites, Inc. |