Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill® PPS F GF/M55 BK 55% Glass/Mineral Filled

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PPS F GF/M55 BK 55% Glass/Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 55% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
ASTM D792
Water Absorption 0.030 %

@Time 86400 sec
0.030 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0025 cm/cm

@Thickness 3.17 mm
0.0025 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 165 MPa
24000 psi
ASTM D638
Elongation at Break 1.5 %
1.5 %
ASTM D638
Flexural Yield Strength 250 MPa
36300 psi
ASTM D790
Flexural Modulus 16.2 GPa
2350 ksi
ASTM D790
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm
1.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 18.0 µm/m-°C
10.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 280 °C
536 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 266 °C
510 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 19.3 kV/mm
490 kV/in
Method A (Short-Time); ASTM D149
Users viewing this material also viewed the following: