Mechanical Properties Metric English Comments
Flexural Modulus 16.2 GPa
2350 ksi
ASTM D790
Oxford Polymers Oxnilon 6-60GF(DRY) PA6, 60% Glass Fiber Reinforced, Dry
Product Description: Glass Fiber (60% Reinforced), Nylon 6 injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents, Lubricants and Heat Stabiliz..
Flexural Modulus 16.2 GPa

@Temperature 115 °C
2350 ksi

@Temperature 239 °F
ASTM D790
Quantum Composites QC-8560 60% Glass Fiber Vinyl Ester SMC
QC-8560 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It maintains excellent mechanical properties at temper..
Flexural Modulus 16.2 GPa
2350 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP KONDUIT OX11315 PPS (Asia Pacific)
Thermally conductive electrically insulative mineral filled PPS FR compound.
Flexural Modulus 16.2 GPa
2350 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP SCP36 PA12
LNP* LUBRICOMP* SCP36 is a compound based on Nylon 12 containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant, Electrically Conductive.
Flexural Modulus 16.2 GPa
2350 ksi
ASTM D790
Techmer ES Electrablend® PA6/6 C20 BK 20% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and LubricatedAppearance: BlackInf..
Flexural Modulus 16.2 GPa
2350 ksi
ASTM D790
Techmer ES Electrablend® PA6/6 CF20 L 20% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Semi Conductive and LubricatedInformation provided by TP C..
Flexural Modulus 16.2 GPa
2350 ksi
ASTM D790
Techmer ES Electrablend® PA6/6 CF20 L BK 20% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and LubricatedAppearance: BlackInf..
Flexural Modulus 16.2 GPa
2350 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI
LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Modulus 16.2 GPa
2350 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP VERTON MV00ES PP
LNP* VERTON* MV00ES is primarily a concentrate used for blending purposes. This is a 70% long glass fiber Polypropylene compound. Added features of this grade are: Heat Stabilized
Flexural Modulus 16.2 GPa
2350 ksi
ASTM D790
Techmer ES HiFill® PPS F GF/M55 BK 55% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 55% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Modulus 16.2 GPa
2350 ksi
ASTM D790
Techmer ES HiFill® PPS GF/M55 BK 55% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 55% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Modulus 16.2 GPa
2350 ksi
ASTM D790
Plenco 6401 Phenolic, Briquette, Transfer Molded
PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco.
Flexural Modulus 16.2 GPa
2350 ksi
ASTM D790
Unitika E-RUNG60 Ultra high-rigidity PA6, Conditioned
Ultra high-rigidityInformation provided by Unitika Ltd.
Flexural Modulus 16.2 GPa
2350 ksi
ASTM D790
A. Schulman ComAlloy Hiloy® 442 Glass Reinforced, PET Alloy
Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 16.2 GPa
2350 ksi
ASTM D570
Solvay Specialty Polymers Xydar® G-430 Glass Filled Liquid Crystal Polymer  (discontinued **)
XYDAR G-430 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electronic applications utilizing surface mount technology at lead-free solder tempe..
Flexural Modulus 16.2 - 16.2 GPa

@Temperature 115 - 115 °C
2350 - 2350 ksi

@Temperature 239 - 239 °F
Average value: 9.03 GPa Grade Count:1