Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 19.3 kV/mm | 490 kV/in | ASTM D149 |
Ravago Manufacturing Americas Hylon® N1040MGHL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 GF13 IM HS BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 GF13 IM2 BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 0135 BL069 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 E GF33 LE 33% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightFeatures: Low ExtractablesProcessing Method: ExtrusionInformation provided by TP Composi.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 GF/M19 HS BK 19% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 19% Filler by Weight and Mineral Filler, 19% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 GF10 L 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 GF13 HS L BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearan.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 GF13 L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 GF14 HS L BK 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearan.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 GF15 TL5 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: PTFE Lubricant (5%)Features: LubricatedAppearance: Natural ColorInformation p.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 GF20 HS BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 GF25 L BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 GF30 HR L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Lubricated and Hydroly.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 GF33 BK 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 GF33 RM L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Low Moisture Absorption and.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 GF33 SL5 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Silicone Lubricant and Heat StabilizerFeatures: Lubricated and Heat Stabilized.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 GF5 HS L 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 GF6 HS BK 6% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 6% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance:.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Luriblend® PA6/6 GF10 M/TL10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: Molybdenum Disulfide Lubricant and PTFE LubricantFeatures: LubricatedAppearance: Natural Col.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | ASTM D149-95 |
Saint-Gobain Tygon® R-3400 UV Resistant Tubing Formulation Tygon® R-3400: Ideal for virtually any permanent or temporary chemical transfer application, Tygon® UV Resistant Tubing combines suppleness and flexibility with resistance to a wide range of.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 GF8 IM3 BK 8% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 8% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubric.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | ASTM D149 |
Ashley Polymers Ashlene® 980LS-33G Nylon 612, 33% Glass Reinforced A 33% glass reinforced, heat stabilized Nylon 612 resin.Data provided by the manufacturer |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Original; ASTM D149-75 |
3M SJ-1FB Cold Shrink Foldback Splice Jacket Kits 3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | ASTM D149 |
Arlon 55560R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for.. |
|||
Dielectric Strength | 19.3 kV/mm | 490 kV/in | Original; ASTM D149-75 |
3M SJ-4FB Cold Shrink Foldback Splice Jacket Kits 3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice.. |
|||
Dielectric Strength | 19.3 - 22.4 kV/mm | 490 - 570 kV/in | Average value: 21.1 kV/mm Grade Count:10 |
Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |