Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill® PA6/6 0137 S2 Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Techmer ES
Trade Name HiFill®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA6/6 0137 S2 Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: High Specific GravityInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ASTM D792
Water Absorption 1.0 %

@Time 86400 sec
1.0 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.016 cm/cm

@Thickness 3.17 mm
0.016 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 72.4 MPa
10500 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 2.83 GPa
410 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm

@Thickness 3.17 mm
0.700 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
280 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C
180 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 10000 - 1.00e+8 ohm-cm
10000 - 1.00e+8 ohm-cm
ASTM D257