Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1000 - 1.00e+8 ohm-cm | 1000 - 1.00e+8 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Hyflon® PFA C920-0020X Perfluoroalkoxy (PFA) Hyflon® PFA C920-0020X is a semi crystalline, melt processable perfluoroalkoxy fluorocarbon resin specifically designed for applications where the unique properties of PFAs must be combined with .. |
|||
Volume Resistivity | 10000 - 1.00e+8 ohm-cm | 10000 - 1.00e+8 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 0137 S2 Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 10000 - 1.00e+8 ohm-cm | 10000 - 1.00e+8 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 0137 S2 Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+6 - 1.00e+8 ohm-cm | 1.00e+6 - 1.00e+8 ohm-cm | ASTM D257 |
Techmer ES Statiblend® POM CO Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeature: ConductiveTPCI# 9962114Information provided by TP Composites, Inc. |
|||
Volume Resistivity | 1000 - 1.00e+8 ohm-cm | 1000 - 1.00e+8 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PA6/6 03003 CF Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Electrically Conductive, Impact.. |
|||
Volume Resistivity | 1000 - 1.00e+8 ohm-cm | 1000 - 1.00e+8 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PA6/6 03004 GF20 Carbon/20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement/Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatu.. |
|||
Volume Resistivity | 1.00e+6 - 1.00e+8 ohm-cm | 1.00e+6 - 1.00e+8 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON LX04420C PEEK LNP* STAT-KON* LX04420C is a compound based on Polyetheretherketone resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding Syst.. |