Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm

@Thickness 3.17 mm
0.0060 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 42.7 MPa
6200 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Yield Strength 58.6 MPa
8500 psi
ASTM D790
Flexural Modulus 2.00 GPa
290 ksi
ASTM D790
Izod Impact, Notched 1.33 J/cm

@Thickness 3.17 mm
2.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 84.4 °C
184 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
ASTM D257