Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 58.6 MPa | 8500 psi | ASTM D790 |
Ineos ABS Lustran® 266 Specialty, Transparent
(discontinued **) A clear injection molding grade of ABS. This transparent, general-purpose grade provides clarity and toughness with ease of processing. Used in housings, toys, lawn and garden applications, and va.. |
|||
Flexural Yield Strength | 58.6 - 207 MPa | 8500 - 30000 psi | Average value: 130 MPa Grade Count:89 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Flexural Yield Strength | 58.6 MPa | 8500 psi | ASTM D790 |
Techmer ES Electrafil® ABS-1251/SD ABS, Static Dissipative Polymer Alloy |
|||
Flexural Yield Strength | 58.6 MPa | 8500 psi | ASTM D790 |
Spartech Royalite R26 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 58.6 MPa | 8500 psi | ASTM D790 |
Star Plastics ABS5035 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 58.6 MPa | 8500 psi | ASTM D790 |
Star Plastics ABSLG5035 Molding Grade ABS, Low Gloss Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 58.6 MPa | 8500 psi | ASTM D790 |
Techmer ES HiFill® PP GF30 LE 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 58.6 MPa @Thickness 3.17 mm |
8500 psi @Thickness 0.125 in |
|
TPI Porene® ABS-GA803 High Gloss, UV Resistant ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 58.6 MPa | 8500 psi | ASTM D790 |
PlastxWorld CEVIAN®-V T150 ABS Medium impact transparent ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |