Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 20 Minutes Milling

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 20 Minutes Milling.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subjected to high wear in service. It has a unique combination of excellent properties, such as low temperature characteristics, and resistance to heat deterioration, ozone cracking, weathering and swelling in oils or solvents.FormulationMillathane CM 100.0N330 Carbon Black30.0Coumarone-Indene Resin15.0MBTS4.0MBT1.0Sulfur0.75CAYTUR 40.35Zinc Stearate0.5All information provided by TSE Industries
Physical Properties Metric English Comments
Mooney Viscosity 42

@Temperature 100 °C
42

@Temperature 212 °F
MS 1+10
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
Tensile Strength, Yield 35.5 MPa
5150 psi
Elongation at Break 580 %
580 %
300% Modulus 0.0128 GPa
1.85 ksi
Tear Strength 62.9 kN/m
359 pli
Die C; ASTM D624
Abrasion 330
330
NBS Index
Compression Set 25 %

@Temperature 70.0 °C,
Time 79200 sec
25 %

@Temperature 158 °F,
Time 22.0 hour
Method B
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 142 °C
1.00 hour

@Temperature 287 °F
Descriptive Properties Value Comments
Mooney Scorch >= 32
at 250ºF; 44 minutes to 10 point rise