Mechanical Properties Metric English Comments
Tear Strength 62.9 kN/m
359 pli
ASTM D624
Multibase Multi-Flex® TPE A 9002 GREY/BROWN
Ash is 15%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tear Strength 63.0 kN/m
359 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 5.0 PHR MBTS
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 62.9 kN/m
359 pli
Die C; ASTM D624
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 20 Minutes Milling
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 63.0 kN/m
359 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR N220 (ISAF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 62.9 kN/m
359 pli
Die C; ASTM D624
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 0.50 PHR Caytur 4
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 62.9 kN/m
359 pli
Die C; ASTM D624
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 20 Minutes Milling
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 63.0 kN/m
359 pli
ASTM Die C
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
Tear Strength 63.0 kN/m
359 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBT
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 63.0 kN/m
359 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 330ºF Cure Temperature
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 63.0 kN/m
359 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 5.0 PHR MBTS
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 63.0 kN/m
359 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Black Sulfur Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 63.0 kN/m
359 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, No Plasticizer
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 63.0 kN/m
359 pli
ASTM Die C
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
Tear Strength 63.0 kN/m
359 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBT
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 63.0 kN/m
359 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 330ºF Cure Temperature
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 63.0 kN/m
359 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, No Plasticizer
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 62.9 kN/m
359 pli
Die C; ASTM D624
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 0.50 PHR Caytur 4
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 63.0 kN/m
359 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR N220 (ISAF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 63.0 kN/m
359 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Black Sulfur Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Copyright © lookpolymers.com All Rights Reserved