Polymer Property : Tensile Strength, Yield = 5150 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.5 MPa
5150 psi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 20 Minutes Milling
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tensile Strength, Yield 35.5 MPa
5150 psi
ASTM D638
Tipco Tipcolene® FPT 40 - 40% Talc Reinforced Polypropylene Homopolymer Compound
40% Talc Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Tensile Strength, Yield 35.5 MPa
5150 psi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 20 Minutes Milling
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tensile Strength, Yield 35.5 MPa
5150 psi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N339 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tensile Strength, Yield 35.5 MPa
5150 psi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N339 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..