Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 300% Modulus = 0.0128 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.0128 GPa
1.85 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N330 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0128 GPa
1.85 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Hercoflex 600 Plasticizer
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0128 GPa
1.85 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Plastolein 9057 Plasticizer
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0128 GPa
1.85 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 15 Minutes Milling
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0128 GPa
1.85 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 20 Minutes Milling
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0128 GPa
1.85 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 5 Minutes Milling
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0128 GPa

@Temperature 145 °C,
Time 2990 sec
1.86 ksi

@Temperature 293 °F,
Time 0.830 hour
cured; ASTM D412
LG Chemical NBR 6250 High Acrylonitrile Polymer
Description: NBR 6250 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6250 is a non staining, medium mooney, an..
300% Modulus 0.0128 GPa
1.85 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Plastolein 9057 Plasticizer
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0128 GPa
1.85 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 15 Minutes Milling
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0128 GPa
1.85 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 20 Minutes Milling
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0128 GPa
1.85 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 78A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.0128 GPa
1.85 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 84A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.0128 GPa
1.85 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N330 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0128 GPa
1.85 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Hercoflex 600 Plasticizer
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0128 GPa
1.85 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 5 Minutes Milling
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0128 GPa
1.86 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4725P General Purpose Molding
FormulationNordel® IP 4725P
300% Modulus 0.0128 GPa
1.86 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR9060 PTMG Polyether Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
300% Modulus 0.0128 GPa
1.85 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 78A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.0128 GPa
1.85 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 84A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
Copyright © lookpolymers.com All Rights Reserved