Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Hercoflex 600 Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Plastolein 9057 Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 15 Minutes Milling MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 20 Minutes Milling MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 5 Minutes Milling MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0127 GPa | 1.85 ksi | 150°C, 40 min., Pressure Vulcanization. 42% Change after 100°C, 70 hrs, Oil Immersion |
KKPC KOSYN KNB 35LL Acrylonitrile Butadiene Rubber (NBR) Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. .. |
|||
300% Modulus | 0.0127 GPa | 1.85 ksi | |
Taiwan Sheen Soon Sheenthane® A8530 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.0127 GPa | 1.85 ksi | |
Taiwan Sheen Soon Sheenthane® A8870E Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.0127 GPa | 1.85 ksi | |
Taiwan Sheen Soon Sheenthane® A8871E2 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.0127 GPa | 1.85 ksi | |
Taiwan Sheen Soon Sheenthane® A8910K Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.0127 GPa | 1.85 ksi | |
Taiwan Sheen Soon Sheenthane® A8915K Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.0127 GPa | 1.85 ksi | |
Taiwan Sheen Soon Sheenthane® A8960N Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.0127 GPa | 1.85 ksi | |
Taiwan Sheen Soon Sheenthane® A8970A Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmWaterproof & breathable gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Plastolein 9057 Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 15 Minutes Milling MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 20 Minutes Milling MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 78A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 84A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Hercoflex 600 Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 5 Minutes Milling MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 78A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 84A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |