Styron CALIBREâ„¢ 891-10 Polycarbonate Resin

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Styron
Trade Name CALIBRE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron CALIBREâ„¢ 891-10 Polycarbonate Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Overview: CALIBREâ„¢ 891-10 Series provides superior ignition resistance in opaque applications. The CALIBRE 891-10 series products are available in 2 additive packages: CALIBRE 891: Mold release, CALIBRE 893: Mold release and UV stabilizer.Main Characteristics: Underwriters Laboratory Inc. (UL) Applications:ElectronicsBusiness equipmentAppliancesInformation provided by Styron
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183/A; ASTM D792
Water Absorption 0.15 %

@Temperature 23.0 °C,
Time 86400 sec
0.15 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ISO 294-4; ASTM D955
Melt Flow 10 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238; ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 59
59
ASTM D785
Hardness, Rockwell R 123
123
ASTM D785
Tensile Strength at Break 58.6 MPa
8500 psi
50 mm/min; ASTM D638
59.0 MPa
8560 psi
ISO 527-2/50
Tensile Strength, Yield 61.0 MPa
8850 psi
ISO 527-2/50
61.4 MPa
8910 psi
50 mm/min; ASTM D638
Elongation at Break 120 %
120 %
50 mm/min; ISO 527-2/50; ASTM D638
Tensile Modulus 5.38 GPa
780 ksi
50 mm/min; ISO 527-2/50; ASTM D638
Flexural Strength 97.9 MPa
14200 psi
Method I (3 point load), 2.0 mm/min; ISO 178; ASTM D790
Flexural Modulus 2.33 GPa
338 ksi
Method I (3 point load), 2.0 mm/min; ISO 178; ASTM D790
Izod Impact, Notched 6.90 J/cm

@Temperature 23.0 °C
12.9 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Izod Impact, Notched (ISO) 68.0 kJ/m²

@Temperature 23.0 °C
32.4 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Tensile Impact Strength 630 kJ/m²
300 ft-lb/in²
ASTM D1822
Dart Drop, Total Energy 62.1 J
45.8 ft-lb
3.39 m/sec; ASTM D3763