Mechanical Properties Metric English Comments
Tensile Modulus 5.38 GPa

@Temperature 175 °C
780 ksi

@Temperature 347 °F
ISO 527-2
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep ..
Tensile Modulus 5.38 GPa
780 ksi
ASTM D638
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th..
Tensile Modulus 5.38 GPa

@Temperature 23.0 °C
780 ksi

@Temperature 73.4 °F
ISO 527-2
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th..
Tensile Modulus 5.38 GPa
780 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics SABIC PPCOMPOUND G3220A PP
SABIC® PPcompound G3220A is a general purpose, 20% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS is 209767996.
Tensile Modulus 5.38 GPa

@Temperature 175 °C
780 ksi

@Temperature 347 °F
4; ISO 527-2
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr..
Tensile Modulus 5.38 GPa
780 ksi
ASTM D638
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry)
Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin..
Tensile Modulus 5.38 GPa
780 ksi
50 mm/min; ISO 527-2/50; ASTM D638
Styron CALIBREâ„¢ 891-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 891-10 Series provides superior ignition resistance in opaque applications. The CALIBRE 891-10 series products are available in 2 additive packages: CALIBRE 891: Mold release..