Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 58.6 MPa | 8500 psi | ASTM D638 |
Oxford Polymers PC 714-FR Series PC, Flame retardant Product Description: Amorphous, Polycarbonate injection molding grade, flame retardant Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents and UV stabilizersSpecial.. |
|||
Tensile Strength at Break | 58.6 MPa | 8500 psi | ASTM D638 |
Ravago Manufacturing Americas Hysun™ A3525 ASA+PC Available in North America Features: Good Impact Resistance RoHS CompliantForm: PelletsInformation provided by Ravago |
|||
Tensile Strength at Break | 58.6 MPa | 8500 psi | TM R050-36 |
Resinlab® EP965 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting .. |
|||
Tensile Strength at Break | 58.6 MPa | 8500 psi | 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® AS-10GF/000 BLACK Acrylonitrile Butadiene Styrene (ABS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Strength at Break | 58.6 MPa | 8500 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 893-10 Polycarbonate Resin Overview: CALIBREâ„¢ 893-10 Series provides superior ignition resistance in opaque applications. The CALIBRE 891-10 series products are available in 2 additive packages: CALIBRE 891: Mold release.. |
|||
Tensile Strength at Break | 58.6 MPa | 8500 psi | ASTM D638 |
Chase Plastics CP Pryme® PC300RUV Polycarbonate (Utility Grade), UV Stabilizer, Mold Release Information provided by Chase Plastics. |
|||
Tensile Strength at Break | 58.6 MPa | 8500 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers NPP25-0802 GF20 20% Glass Filled Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength at Break | >= 58.6 MPa | >= 8500 psi | |
Master Bond EP33LV Epoxy Has Dimensional Stability and Machinability Description: Master Bond EP33LV is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and very g.. |