Material Notes:
CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact strength. The CALIBRE 300 series can be supplied with a mold release package, a UV stabilizer package or both.The CALIBRE 300 series resins are typically used for appliances, storage media housings, extruded sheet, electrical components and lighting.Available Melt Flow Rates: 4, 6, 10, 15.Associated products: CALIBRE 300: without a mold release and UV stabilization package CALIBRE 301: including a mold release package CALIBRE 302: including a UV stabilizer package CALIBRE 303: including a mold release and UV stabilizer package.Data provided by Dow Chemical.This product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM Data
Melt Density 1.00 g/cc
0.0361 lb/in³
Melt density
Water Absorption 0.15 %
0.15 %
Moisture Absorption at Equilibrium 0.32 %
0.32 %
Humidity Absorption
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Melt Flow 4.0 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
4.0 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
ASTM Data
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
Tensile Strength, Ultimate 72.4 MPa
10500 psi
ASTM Data
Tensile Strength, Yield 62.1 MPa
9010 psi
ASTM Data
Elongation at Break 150 %
150 %
ASTM Data
Elongation at Yield 6.0 %
6.0 %
ISO Data
Tensile Modulus 2.48 GPa
360 ksi
ASTM Data
Izod Impact, Notched 9.61 J/cm
18.0 ft-lb/in
ASTM Data
Izod Impact, Unnotched NB
NB
ASTM Data
Charpy Impact Unnotched NB
NB
ISO Data
NB
NB
ISO Data, Low Temp
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
ISO Data, Low Temp
10.0 J/cm²
47.6 ft-lb/in²
ISO Data
Tensile Impact Strength 631 kJ/m²
300 ft-lb/in²
ASTM Data
Impact Test 93.8 J
<br>@Temperature 23.0 °C
69.2 ft-lb
<br>@Temperature 73.4 °F
Instrumented Dart Total Energy
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 68.4 µm/m-°C
<br>@Temperature 20.0 °C
38.0 µin/in-°F
<br>@Temperature 68.0 °F
ASTM data
Specific Heat Capacity 1.96 J/g-°C
0.468 BTU/lb-°F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
Unannealed; ASTM Data
Vicat Softening Point 158 °C
316 °F
Flammability, UL94 V-2
<br>@Thickness 3.20 mm
V-2
<br>@Thickness 0.126 in
Oxygen Index 26 %
26 %
Optical Properties Metric English Comments
Haze 1.1 %
1.1 %
Transmission, Visible 89 %
89 %
Electrical Properties Metric English Comments
Electrical Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM Data
Dielectric Constant 2.93
<br>@Frequency 60 Hz
2.93
<br>@Frequency 60 Hz
ASTM Data
2.93
<br>@Frequency 1e+6 Hz
2.93
<br>@Frequency 1e+6 Hz
ASTM Data
Dielectric Strength 16.5 kV/mm
419 kV/in
Dissipation Factor 0.00050
<br>@Frequency 60 Hz
0.00050
<br>@Frequency 60 Hz
0.0017
<br>@Frequency 1e+6 Hz
0.0017
<br>@Frequency 1e+6 Hz
ASTM Data