ApplicationsPETROTHENE XL07425 is especially formulated for use in flame retardant primary insulation for low voltage automotive wire and cable applications (SAE J1128). Non-discoloring antioxidant and special active peroxide have been added to ensure thermal stability during processing and optimum curing results.Processing TechniquesXL07425, like other crosslinkable polyolefin compounds, can be extruded as wire and cable insulation by means of a conventional extruder with a continuous vulcanization tube. Below are suggested extrusion and curing conditions for XL07425. These conditions are intended as general guidelines only, and not optimum values, since manufacturing variables such as extruder type and size, continuous vulcanization tube design and cable construction all have an effect on processing crosslinkable compounds. Contact your Equistar sales representative for more information.Additional SuggestionsMaximum screen pack of 40 meshLittle or no die landNo predrying normally requiredCompression ratio of 2:1-3:1"Mixing" screw can be used if properly designed to prevent excessive heat build-upDies should be cleaned frequently to reduce compound build-upOn-size dies are recommendedCuring line steam temperature should be at least 400°F (205°C)Physical PropertiesAll properties determined from compression molded, press cured plaques. The values listed for physical properties are nominal values only and are subject to normal variations consistent with the test methods and/or variations found acceptable to the industry.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D1505
Mechanical Properties Metric English Comments
Hardness, Shore D 56
56
ASTM D2240
Tensile Strength at Break 19.4 MPa
2810 psi
106% retained after aging 7 days at 165°C; ASTM D412
Elongation at Break 250 %
250 %
97% retained after aging 7 days at 165°C; ASTM D412
Thermal Properties Metric English Comments
Oxygen Index 25 %
25 %
ASTM D2863
Processing Properties Metric English Comments
Feed Temperature 107 - 113 °C
225 - 235 °F
Zone 2 107 - 113 °C
225 - 235 °F
Zone 3 107 - 113 °C
225 - 235 °F
Zone 3-X
Adapter Temperature 113 - 118 °C
235 - 245 °F
Melt Temperature 116 - 127 °C
240 - 260 °F
Head Temperature 113 - 118 °C
235 - 245 °F
Screw Cooling Temperature 82.2 °C
180 °F
If needed
Die Cooling Temperature 32.2 - 48.9 °C
90.0 - 120 °F